Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Aremco Corr-Paint™ CP4040 High Temperature Protective Coating Silicone

Category Other Engineering Material , Ceramic/Metallic Coating , Polymer , Thermoset , Silicone
Manufacturer Aremco
Trade Name Corr-Paint™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aremco Corr-Paint™ CP4040 High Temperature Protective Coating Silicone.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Low viscosity, white coating for motor windings to 1100°F (593°C)
Physical Properties Metric English Comments
Specific Gravity 1.27 g/cc
1.27 g/cc
Solids Content 44.2 %
44.2 %
by weight
46.1 %
46.1 %
by volume
Volatile Organic Compounds (VOC) Content 117 g/l
117 g/l
Viscosity 400 - 900 cP
400 - 900 cP
Thickness 38.1 microns
1.50 mil
recommended dry film thickness
102 microns
4.00 mil
estimated wet film thickness
Storage Temperature 12.8 - 29.4 °C
55.0 - 85.0 °F
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 593 °C
1100 °F
Flash Point >= 100 °C
>= 212 °F
Electrical Properties Metric English Comments
Dielectric Strength 12.2 kV/mm
310 kV/in
Processing Properties Metric English Comments
Processing Temperature 10.0 - 48.9 °C
50.0 - 120 °F
Application Temperature
Cure Time >= 60.0 min
>= 1.00 hour
Air Set prior to curing
45.0 min

@Temperature 232 °C
0.750 hour

@Temperature 450 °F
Adequate ventilation is required when curing these products. Outgassing will occur above 300°F and cease after 750°F. An additional 30 minutes is required at the highest service temperature if service temperature is below 750°F.
Shelf Life 6.00 Month
6.00 Month
Descriptive Properties Value Comments
Color White
Dry Film Coverage ft2/gal 740
at 1 mil
Thinner Butyl Cellosolve/Water
Copyright © lookpolymers.com All Rights Reserved