Plenco 7466 Phenolic, Nodular, Injection Molded  (discontinued **)

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic , Phenolic, Novolac, Mineral/Flock Filled
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 7466 Phenolic, Nodular, Injection Molded  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Two-Stage Phenolic. PLENCO 07466 is a flock cotton and mineral filled phenolic molding compound offering excellent heat resistance and dimensional stability. UL recognized under component file E40654. 07466 is available in black.Information supplied by Plenco
Physical Properties Metric English Comments
Density 1.58 g/cc
0.0571 lb/in³
ASTM D792
Apparent Bulk Density 0.670 g/cc
0.0242 lb/in³
Apparent density per ASTM D1895
Water Absorption 0.15 %
0.15 %
ASTM D570
Linear Mold Shrinkage 0.0058 cm/cm
0.0058 in/in
per ATM D955. Post shrinkage is 0.15% at 72hr 120ºC per ASTM D1299.
Mechanical Properties Metric English Comments
Hardness, Rockwell E 82
82
ASTM D785
Tensile Strength, Ultimate 51.8 MPa
7510 psi
ASTM D638
Elongation at Break 0.59 %
0.59 %
ASTM D638
Tensile Modulus 10.08 GPa
1462 ksi
ASTM D638
Flexural Yield Strength 84.0 MPa
12200 psi
ASTM D790
Flexural Modulus 9.08 GPa
1320 ksi
ASTM D790
Compressive Yield Strength 191.6 MPa
27790 psi
ASTM D695
Poissons Ratio 0.33
0.33
In tension
Shear Modulus 3.80 GPa
551 ksi
Calculated
Charpy Impact, Notched 0.200 J/cm²
0.952 ft-lb/in²
ASTM D256
Impact 122
122
J/m Plenco drop ball test
Thermal Properties Metric English Comments
CTE, linear 30.0 µm/m-°C

@Temperature 20.0 °C
16.7 µin/in-°F

@Temperature 68.0 °F
Maximum Service Temperature, Air 203 °C
397 °F
Heat resistance per ASTM D794
Deflection Temperature at 1.8 MPa (264 psi) 177 °C
351 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 1.47 mm
V-0

@Thickness 0.0579 in
Electrical Properties Metric English Comments
Electrical Resistivity 4.01e+11 ohm-cm
4.01e+11 ohm-cm
ASTM D257
Dielectric Constant 5.0

@Frequency 1e+6 Hz
5.0

@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 12.2 kV/mm
310 kV/in
Short Time; ASTM D149
Dissipation Factor 0.049

@Frequency 1e+6 Hz
0.049

@Frequency 1e+6 Hz
ASTM D150
Arc Resistance 180 sec
180 sec
ASTM D495
Comparative Tracking Index 175 V
175 V
ASTM D3638