Solvay TECHNYL® A 216 V20 PA66, 20% glass fiber, Conditioned

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 20% Glass Fiber Filled
Manufacturer Solvay
Trade Name Technyl®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay TECHNYL® A 216 V20 PA66, 20% glass fiber, Conditioned.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Polyamide 66, reinforced with 20% of glass fiber, for injection molding.Available in: Europe Product Applications: TECHNYL® A 216 V20 is used in all sectors of industry, offering and excellent combination between thermal and mechanical properties. This grade is used in: Automotive industry, Manufacture of components for electrical tools and Transport and building. This product is available in natural and black, and in a wide range of standard colors.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.29 g/cc
0.0466 lb/in³
ISO 1183/A
Mechanical Properties Metric English Comments
Tensile Strength at Break 100 MPa
14500 psi
ISO 527 Type 1A
Elongation at Break 5.0 %
5.0 %
ISO 527 Type 1A
Tensile Modulus 5.30 GPa
769 ksi
ISO 527 Type 1A
Flexural Modulus 4.20 GPa
609 ksi
ISO 178
Izod Impact, Notched (ISO) 13.0 kJ/m²
6.19 ft-lb/in²
ISO 180/1A
Charpy Impact Unnotched 7.90 J/cm²
37.6 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 1.00 J/cm²
4.76 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 30.0 µm/m-°C

@Temperature 23.0 - 85.0 °C
16.7 µin/in-°F

@Temperature 73.4 - 185 °F
ISO 11359
Electrical Properties Metric English Comments
Volume Resistivity 2.00e+12 ohm-cm
2.00e+12 ohm-cm
IEC 60093
Surface Resistance 1.00e+11 ohm
1.00e+11 ohm
IEC 60093
Dielectric Constant 4.0
4.0
IEC 60250
Dielectric Strength 28.0 kV/mm
711 kV/in
IEC 60243
Dissipation Factor 0.11
0.11
IEC 60250
Comparative Tracking Index 525 V
525 V
Solution B; IEC 60112
600 V
600 V
Solution A; IEC 60112
Processing Properties Metric English Comments
Moisture Content <= 0.20 %
<= 0.20 %