Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Geon™ Vinyl Wire & Cable W9200 Polyvinyl Chloride, Flexible (PVC, Flexible)

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer PolyOne Corporation
Trade Name Geon™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Geon™ Vinyl Wire & Cable W9200 Polyvinyl Chloride, Flexible (PVC, Flexible).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.32 g/cc
1.32 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore D 77
77
ASTM D2240
Tensile Strength at Break 28.3 MPa
4100 psi
Type IV, 510 mm/min; ASTM D638
Elongation at Break 230 %
230 %
Type IV, 510 mm/min; ASTM D638
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 105 °C
221 °F
UL Temperature Rating
Oxygen Index 28 %

@Thickness 1.91 mm
28 %

@Thickness 0.0752 in
ASTM D2863
Electrical Properties Metric English Comments
Volume Resistivity 5.00e+12 ohm-cm
5.00e+12 ohm-cm
ASTM D257
Dielectric Constant 3.3

@Frequency 1000 Hz
3.3

@Frequency 1000 Hz
ASTM D150
Dielectric Strength 28.0 kV/mm
711 kV/in
ASTM D149
Descriptive Properties Value Comments
Additive Lead Stabilizer
Features Flame Retardant
Forms Pellets
Generic Material PVC, Flexible
Generic Name Polyvinyl Chloride, Flexible (PVC, Flexible)
Processing Method Extrusion Coating
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Communication Wire Insulation
Wire & Cable Applications