Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

EMS-Grivory Grivory® EB 50 H PA6

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer EMS-Grivory (EMS-CHEMIE)
Trade Name Grivory®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF EMS-Grivory Grivory® EB 50 H PA6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product description: Grilon EB 50 H is a high viscosity, unreinforced, heat stabilized PA6 extrusion blow mounding grade. Grilon EB 50 H has the following important properties: High melt strengthImpact resistant even at low temperaturesProcessable on conventional as well as on 3 D-machines Grilon EB 50 H is used typically for automotive applications such are air ducts for turbochargers, air ducts, oil filler pipes, fuel and oil containers.Information provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.11 g/cc
0.0401 lb/in³
ISO 1183
Water Absorption 9.0 %
9.0 %
ISO 62
Moisture Absorption 3.00 %
3.00 %
ISO 62
Mechanical Properties Metric English Comments
Ball Indentation Hardness 55.0 MPa
7980 psi
conditioned; ISO 2039-1
135 MPa
19600 psi
dry; ISO 2039-1
Tensile Strength at Break 50.0 MPa
7250 psi
dry; ISO 527-1/-2
50.0 MPa
7250 psi
conditioned; ISO 527-1/-2
Tensile Strength, Yield 40.0 MPa
5800 psi
dry; ISO 527-1/-2
75.0 MPa
10900 psi
dry; ISO 527-1/-2
Elongation at Break >= 50 %
>= 50 %
conditioned; ISO 527-1/-2
<= 50 %
<= 50 %
dry; ISO 527-1/-2
Elongation at Yield 4.0 %
4.0 %
dry; ISO 527-1/-2
20 %
20 %
conditioned; ISO 527-1/-2
Tensile Modulus 0.800 GPa
116 ksi
conditioned; ISO 527-1/-2
2.80 GPa
406 ksi
dry; ISO 527-1/-2
Charpy Impact Unnotched NB
NB
dry; ISO 179/1eU
NB
NB
conditioned; ISO 179/1eU
NB

@Temperature 30.0 °C
NB

@Temperature 86.0 °F
dry; ISO 179/1eU
NB

@Temperature 30.0 °C
NB

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Charpy Impact, Notched 1.10 J/cm²
5.23 ft-lb/in²
dry; ISO 179/1eA
NB
NB
conditioned; ISO 179/1eA
0.900 J/cm²

@Temperature 30.0 °C
4.28 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
1.00 J/cm²

@Temperature 30.0 °C
4.76 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 90.0 µm/m-°C
50.0 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 120 µm/m-°C
66.7 µin/in-°F
ISO 11359-1/-2
Melting Point 222 °C
432 °F
10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 100 - 120 °C
212 - 248 °F
long term; EMS
180 °C
356 °F
short term; EMS
Deflection Temperature at 0.46 MPa (66 psi) 140 °C
284 °F
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °C
131 °F
ISO 75-1/-2
Flammability, UL94 HB
HB
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
conditioned; IEC 60093
1.00e+13 ohm-cm
1.00e+13 ohm-cm
dry; IEC 60093
Surface Resistance 1.00e+10 ohm
1.00e+10 ohm
IEC 60093
Dielectric Strength 24.0 kV/mm
610 kV/in
conditioned; IEC 60243-1
28.0 kV/mm
711 kV/in
dry; IEC 60243-1
Comparative Tracking Index 425 V
425 V
conditioned; IEC 60112
Descriptive Properties Value Comments
Automotive Air intake sytems
Cooling and climate control
Electricals & Electronics Cables & Tubes
Form Granules
Industry & Consumer goods Hydraulics & Pneumatics
Processing Extrusion - blow molding
Other Extrusion
Special Characteristics Improved heat resistance