Electrical Properties | Metric | English | Comments |
---|---|---|---|
Arc Resistance | 120 - 190 sec | 120 - 190 sec | Average value: 124 sec Grade Count:18 |
Overview of materials for Thermoset Polyurethane, Adhesive This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Adhesive". Each property range of values reported is minimum and maximum values .. |
|||
Arc Resistance | 18.0 - 190 sec | 18.0 - 190 sec | Average value: 161 sec Grade Count:7 |
Overview of materials for Epoxy, Molded, Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Molded, Mineral Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Arc Resistance | 178 - 190 sec | 178 - 190 sec | Average value: 181 sec Grade Count:12 |
Overview of materials for Epoxy, Encapsulating, Glass or Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Encapsulating, Glass or Mineral Filled". Each property range of values reported is minimum and ma.. |
|||
Arc Resistance | 120 - 190 sec | 120 - 190 sec | Average value: 145 sec Grade Count:8 |
Overview of materials for Phenolic; Unreinforced; Molded This property data is a summary of similar materials in the MatWeb database for the category "Phenolic; Unreinforced; Molded". Each property range of values reported is minimum and maximum values of.. |
|||
Arc Resistance | 181 - 190 sec | 181 - 190 sec | Average value: 185 sec Grade Count:3 |
Overview of materials for Phenolic, Resole, Mineral/Flock Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Resole, Mineral/Flock Filled". Each property range of values reported is minimum and maximum v.. |
|||
Arc Resistance | 185 - 190 sec | 185 - 190 sec | ASTM D495 |
Hexion Bakelite™ PF 4109 Phenolic Formaldehyde Resin, Improved Electrical Properties, Ammonia Free, Resistant to High Temperatures, Low Shrinkage, High Arc Resistance, UL Listed, Acetic Acid Free Phenolic molding compound, inorganically filled, glass fiber reinforced, ammonia and acetic acid free, electrically high grade, high temperature stability, low shrinkage, high mechanical strength, U.. |
|||
Arc Resistance | 115 - 190 sec | 115 - 190 sec | Average value: 138 sec Grade Count:6 |
Overview of materials for Nylon 6, 40% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Mineral Filled". Each property range of values reported is minimum and maximum values of ap.. |
|||
Arc Resistance | 180 - 190 sec | 180 - 190 sec | |
Bulk Molding Compounds BMC 6241 Glass Fiber Reinforced Compound BMC 6241 is a glass fiber-reinforced material formulated specifically for molding of industrial lighting reflectors where adequate strength is required along with a high reflectivity. It is availabl.. |
|||
Arc Resistance | 180 - 190 sec | 180 - 190 sec | |
Bulk Molding Compounds BMC 6241 Glass Reinforced BMC BMC 6241 is a glass fiber-reinforced material formulated specifically for molding of industrial lighting reflectors where adequate strength is required along with a high reflectivity. It is availab.. |
|||
Arc Resistance | 180 - 190 sec | 180 - 190 sec | |
Bulk Molding Compounds BMC 900 Thermoset Polyester, Soft Flow Encapsulation Grade BMC 900 is an encapsulation grade, soft flow material. As with all other BMCI compounds, this series can be supplied in logs, slugs or bulk.Typical applications are electrical coil encapsulations an.. |
|||
Arc Resistance | 185 - 190 sec | 185 - 190 sec | ASTM D495 |
Hexion Bakelite™ PF 4111 Phenolic Formaldehyde Resin, Improved Electrical Properties, Ammonia Free, Resistant to High Temperatures, Low Shrinkage, High Arc Resistance, UL Listed, Acetic Acid Free, Copper Adhesive Phenolic molding compound, inorganically filled, glass fiber reinforced, ammonia and acetic acid free, electrically high grade, high temperature stability, high mechanical strength, copper-adhesive,.. |
|||
Arc Resistance | 180 - 190 sec | 180 - 190 sec | ASTM D495-61 |
Bulk Molding Compounds tetra-DUR F 4306 Bulk Molding Compound Mechanical high grade standard productTypical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipation (explosion pr.. |