Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Overview of materials for Phenolic, Resole, Mineral/Flock Filled

Category Polymer , Thermoset , Phenolic , Phenolic, Resole, Mineral/Flock Filled
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Phenolic, Resole, Mineral/Flock Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Resole, Mineral/Flock Filled". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.56 - 1.59 g/cc
0.0564 - 0.0574 lb/in³
Average value: 1.58 g/cc Grade Count:3
Water Absorption 0.400 - 0.560 %
0.400 - 0.560 %
Average value: 0.477 % Grade Count:3
Linear Mold Shrinkage 0.00340 - 0.00530 cm/cm
0.00340 - 0.00530 in/in
Average value: 0.00430 cm/cm Grade Count:3
Mechanical Properties Metric English Comments
Hardness, Rockwell E 57.0 - 67.0
57.0 - 67.0
Average value: 62.0 Grade Count:3
Tensile Strength, Ultimate 51.1 - 58.0 MPa
7410 - 8410 psi
Average value: 54.0 MPa Grade Count:3
Elongation at Break 0.800 - 1.11 %
0.800 - 1.11 %
Average value: 0.920 % Grade Count:3
Modulus of Elasticity 8.70 - 10.1 GPa
1260 - 1460 ksi
Average value: 9.43 GPa Grade Count:3
Flexural Yield Strength 79.0 - 83.0 MPa
11500 - 12000 psi
Average value: 80.5 MPa Grade Count:3
Flexural Modulus 8.01 - 9.20 GPa
1160 - 1330 ksi
Average value: 8.60 GPa Grade Count:3
Compressive Yield Strength 139 - 163 MPa
20200 - 23600 psi
Average value: 155 MPa Grade Count:3
Izod Impact, Notched 0.190 - 0.271 J/cm
0.356 - 0.508 ft-lb/in
Average value: 0.224 J/cm Grade Count:3
Charpy Impact, Notched 0.205 - 0.251 J/cm²
0.976 - 1.19 ft-lb/in²
Average value: 0.222 J/cm² Grade Count:3
Thermal Properties Metric English Comments
CTE, linear 34.0 - 34.0 µm/m-°C

@Temperature 40.0 - 130 °C
18.9 - 18.9 µin/in-°F

@Temperature 104 - 266 °F
Average value: 34.0 µm/m-°C Grade Count:1
Thermal Conductivity 0.550 - 0.550 W/m-K

@Temperature 100 - 100 °C
3.82 - 3.82 BTU-in/hr-ft²-°F

@Temperature 212 - 212 °F
Average value: 0.550 W/m-K Grade Count:1
Maximum Service Temperature, Air 188 - 210 °C
370 - 410 °F
Average value: 200 °C Grade Count:3
Deflection Temperature at 1.8 MPa (264 psi) 199 - 240 °C
390 - 464 °F
Average value: 214 °C Grade Count:3
Flammability, UL94 V-1 - V-0
V-1 - V-0
Grade Count:3
Electrical Properties Metric English Comments
Electrical Resistivity 2.02e+11 - 1.70e+12 ohm-cm
2.02e+11 - 1.70e+12 ohm-cm
Average value: 7.97e+11 ohm-cm Grade Count:3
Dielectric Constant 6.50 - 7.90
6.50 - 7.90
Average value: 7.40 Grade Count:3
Dielectric Strength 6.90 - 9.40 kV/mm
175 - 239 kV/in
Average value: 7.90 kV/mm Grade Count:3
Dissipation Factor 0.0990 - 0.162
0.0990 - 0.162
Average value: 0.127 Grade Count:3
Arc Resistance 181 - 190 sec
181 - 190 sec
Average value: 185 sec Grade Count:3
Comparative Tracking Index 175 - 200 V
175 - 200 V
Average value: 192 V Grade Count:3