Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Arc Resistance = 190 sec Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Arc Resistance 120 - 190 sec
120 - 190 sec
Average value: 124 sec Grade Count:18
Overview of materials for Thermoset Polyurethane, Adhesive
This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Adhesive". Each property range of values reported is minimum and maximum values ..
Arc Resistance 18.0 - 190 sec
18.0 - 190 sec
Average value: 161 sec Grade Count:7
Overview of materials for Epoxy, Molded, Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Molded, Mineral Filled". Each property range of values reported is minimum and maximum values of ..
Arc Resistance 178 - 190 sec
178 - 190 sec
Average value: 181 sec Grade Count:12
Overview of materials for Epoxy, Encapsulating, Glass or Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Encapsulating, Glass or Mineral Filled". Each property range of values reported is minimum and ma..
Arc Resistance 120 - 190 sec
120 - 190 sec
Average value: 145 sec Grade Count:8
Overview of materials for Phenolic; Unreinforced; Molded
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic; Unreinforced; Molded". Each property range of values reported is minimum and maximum values of..
Arc Resistance 181 - 190 sec
181 - 190 sec
Average value: 185 sec Grade Count:3
Overview of materials for Phenolic, Resole, Mineral/Flock Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Resole, Mineral/Flock Filled". Each property range of values reported is minimum and maximum v..
Arc Resistance 185 - 190 sec
185 - 190 sec
ASTM D495
Hexion Bakelite™ PF 4109 Phenolic Formaldehyde Resin, Improved Electrical Properties, Ammonia Free, Resistant to High Temperatures, Low Shrinkage, High Arc Resistance, UL Listed, Acetic Acid Free
Phenolic molding compound, inorganically filled, glass fiber reinforced, ammonia and acetic acid free, electrically high grade, high temperature stability, low shrinkage, high mechanical strength, U..
Arc Resistance 115 - 190 sec
115 - 190 sec
Average value: 138 sec Grade Count:6
Overview of materials for Nylon 6, 40% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Mineral Filled". Each property range of values reported is minimum and maximum values of ap..
Arc Resistance 180 - 190 sec
180 - 190 sec
Bulk Molding Compounds BMC 6241 Glass Fiber Reinforced Compound
BMC 6241 is a glass fiber-reinforced material formulated specifically for molding of industrial lighting reflectors where adequate strength is required along with a high reflectivity. It is availabl..
Arc Resistance 180 - 190 sec
180 - 190 sec
Bulk Molding Compounds BMC 6241 Glass Reinforced BMC
BMC 6241 is a glass fiber-reinforced material formulated specifically for molding of industrial lighting reflectors where adequate strength is required along with a high reflectivity. It is availab..
Arc Resistance 180 - 190 sec
180 - 190 sec
Bulk Molding Compounds BMC 900 Thermoset Polyester, Soft Flow Encapsulation Grade
BMC 900 is an encapsulation grade, soft flow material. As with all other BMCI compounds, this series can be supplied in logs, slugs or bulk.Typical applications are electrical coil encapsulations an..
Arc Resistance 185 - 190 sec
185 - 190 sec
ASTM D495
Hexion Bakelite™ PF 4111 Phenolic Formaldehyde Resin, Improved Electrical Properties, Ammonia Free, Resistant to High Temperatures, Low Shrinkage, High Arc Resistance, UL Listed, Acetic Acid Free, Copper Adhesive
Phenolic molding compound, inorganically filled, glass fiber reinforced, ammonia and acetic acid free, electrically high grade, high temperature stability, high mechanical strength, copper-adhesive,..
Arc Resistance 180 - 190 sec
180 - 190 sec
ASTM D495-61
Bulk Molding Compounds tetra-DUR F 4306 Bulk Molding Compound
Mechanical high grade standard productTypical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipation (explosion pr..
Copyright © lookpolymers.com All Rights Reserved