Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Overview of materials for Thermoset Polyurethane, Adhesive

Category Polymer , Adhesive , Thermoset , Polyurethane, TS , Thermoset Polyurethane, Adhesive
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Thermoset Polyurethane, Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Adhesive". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 0.780 - 3.20 g/cc
0.0282 - 0.116 lb/in³
Average value: 1.21 g/cc Grade Count:77
Volatile Organic Compounds (VOC) Content 2.10 - 510 g/l
2.10 - 510 g/l
Average value: 222 g/l Grade Count:13
Water Absorption 0.0600 - 0.400 %
0.0600 - 0.400 %
Average value: 0.215 % Grade Count:25
Moisture Absorption at Equilibrium 0.150 - 0.180 %
0.150 - 0.180 %
Average value: 0.157 % Grade Count:4
Water Absorption at Saturation 0.00150 - 0.0120 %
0.00150 - 0.0120 %
Average value: 0.00427 % Grade Count:17
Loss On Ignition 0.0500 - 0.570 %

@Temperature 100 - 130 °C
0.0500 - 0.570 %

@Temperature 212 - 266 °F
Average value: 0.304 % Grade Count:4
0.0500 - 0.570 %

@Time 86400 - 605000 sec
0.0500 - 0.570 %

@Time 24.0 - 168 hour
Average value: 0.304 % Grade Count:4
Viscosity 30.0 - 1.20e+6 cP
30.0 - 1.20e+6 cP
Average value: 28200 cP Grade Count:88
600 - 600 cP

@Temperature 50.0 - 50.0 °C
600 - 600 cP

@Temperature 122 - 122 °F
Average value: 600 cP Grade Count:1
Linear Mold Shrinkage 0.000500 - 0.0125 cm/cm
0.000500 - 0.0125 in/in
Average value: 0.00805 cm/cm Grade Count:21
Outgassing - Total Mass Loss 0.150 - 2.50 %
0.150 - 2.50 %
Average value: 0.544 % Grade Count:14
Mechanical Properties Metric English Comments
Hardness, Shore A 10.0 - 95.0
10.0 - 95.0
Average value: 58.6 Grade Count:52
75.0 - 75.0

@Temperature -40.0 - -40.0 °C
75.0 - 75.0

@Temperature -40.0 - -40.0 °F
Average value: 75.0 Grade Count:2
Hardness, Shore D 35.0 - 75.0
35.0 - 75.0
Average value: 56.3 Grade Count:26
Hardness, Shore OO 50.0 - 65.0
50.0 - 65.0
Average value: 60.0 Grade Count:3
Tensile Strength, Ultimate 0.0689 - 29.0 MPa
10.0 - 4210 psi
Average value: 9.80 MPa Grade Count:58
Tensile Strength, Yield 0.0345 - 11.7 MPa
5.00 - 1700 psi
Average value: 1.32 MPa Grade Count:17
Elongation at Break 30.0 - 874 %
30.0 - 874 %
Average value: 345 % Grade Count:61
Elongation at Yield 68.0 - 250 %
68.0 - 250 %
Average value: 204 % Grade Count:4
Modulus of Elasticity 0.0000345 - 0.0896 GPa
0.00500 - 13.0 ksi
Average value: 0.0331 GPa Grade Count:23
0.00413685 - 0.00413685 GPa

@Temperature 55.0 - 55.0 °C
0.600009 - 0.600009 ksi

@Temperature 131 - 131 °F
Average value: 0.00414 GPa Grade Count:1
Compressive Yield Strength 0.0345 - 19.1 MPa
5.00 - 2780 psi
Average value: 3.73 MPa Grade Count:3
Shear Strength 0.352 - 13.8 MPa
51.0 - 2000 psi
Average value: 3.99 MPa Grade Count:7
0.690 - 17.2 MPa

@Temperature -55.0 - 121 °C
100 - 2490 psi

@Temperature -67.0 - 250 °F
Average value: 5.90 MPa Grade Count:4
Adhesive Bond Strength 0.138 - 20.7 MPa
20.0 - 3000 psi
Average value: 4.69 MPa Grade Count:18
Tear Strength 6.14 - 56.1 kN/m
35.0 - 320 pli
Average value: 32.9 kN/m Grade Count:9
Thermal Properties Metric English Comments
CTE, linear 1.00 - 510 µm/m-°C
0.556 - 283 µin/in-°F
Average value: 161 µm/m-°C Grade Count:43
Thermal Conductivity 0.140 - 1.76 W/m-K
0.972 - 12.2 BTU-in/hr-ft²-°F
Average value: 0.570 W/m-K Grade Count:22
Maximum Service Temperature, Air 51.7 - 150 °C
125 - 302 °F
Average value: 109 °C Grade Count:59
Minimum Service Temperature, Air -65.0 - -30.0 °C
-85.0 - -22.0 °F
Average value: -52.0 °C Grade Count:48
Glass Transition Temp, Tg -83.0 - 71.0 °C
-117 - 160 °F
Average value: -34.4 °C Grade Count:34
Flash Point -1.11 - 200 °C
30.0 - 392 °F
Average value: 90.3 °C Grade Count:34
Optical Properties Metric English Comments
Transmission, Visible 90.0 %
90.0 %
Average value: 90.0 % Grade Count:9
Electrical Properties Metric English Comments
Electrical Resistivity 0.00500 - 2.00e+16 ohm-cm
0.00500 - 2.00e+16 ohm-cm
Average value: 2.38e+15 ohm-cm Grade Count:54
1.30e+10 - 4.00e+14 ohm-cm

@Temperature 65.0 - 130 °C
1.30e+10 - 4.00e+14 ohm-cm

@Temperature 149 - 266 °F
Average value: 5.00e+13 ohm-cm Grade Count:8
Surface Resistance 3.50e+6 - 6.10e+17 ohm
3.50e+6 - 6.10e+17 ohm
Average value: 4.71e+16 ohm Grade Count:19
Insulation Resistance 3.20e+12 - 4.50e+14 ohm
3.20e+12 - 4.50e+14 ohm
Average value: 1.30e+14 ohm Grade Count:17
Dielectric Constant 2.67 - 5.90
2.67 - 5.90
Average value: 3.74 Grade Count:59
3.18 - 3.50

@Temperature -40.0 - 140 °C
3.18 - 3.50

@Temperature -40.0 - 284 °F
Average value: 3.34 Grade Count:1
3.18 - 3.50

@Frequency 1.00e+6 - 1.00e+6 Hz
3.18 - 3.50

@Frequency 1.00e+6 - 1.00e+6 Hz
Average value: 3.34 Grade Count:1
Dielectric Strength 13.4 - 138 kV/mm
340 - 3500 kV/in
Average value: 37.9 kV/mm Grade Count:51
Dielectric Breakdown 1500 V
1500 V
Average value: 1500 V Grade Count:7
Dissipation Factor 0.00900 - 0.200
0.00900 - 0.200
Average value: 0.0365 Grade Count:51
0.00500 - 0.0700

@Temperature -40.0 - 140 °C
0.00500 - 0.0700

@Temperature -40.0 - 284 °F
Average value: 0.0375 Grade Count:1
0.00500 - 0.0700

@Frequency 1.00e+6 - 1.00e+6 Hz
0.00500 - 0.0700

@Frequency 1.00e+6 - 1.00e+6 Hz
Average value: 0.0375 Grade Count:1
Arc Resistance 120 - 190 sec
120 - 190 sec
Average value: 124 sec Grade Count:18
Processing Properties Metric English Comments
Processing Temperature 4.00 - 125 °C
39.2 - 257 °F
Average value: 83.5 °C Grade Count:29
Cure Time 3.00 - 43200 min
0.0500 - 720 hour
Average value: 4860 min Grade Count:57
5.00 - 20160 min

@Temperature 60.0 - 190 °C
0.0833 - 336.0 hour

@Temperature 140 - 374 °F
Average value: 1180 min Grade Count:44
Pot Life 1.50 - 600 min
1.50 - 600 min
Average value: 41.7 min Grade Count:59
40.0 - 50.0 min

@Temperature 50.0 - 50.0 °C
40.0 - 50.0 min

@Temperature 122 - 122 °F
Average value: 45.0 min Grade Count:1
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved