Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plenco 1501 Polyester, Briquette, Transfer Molded

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Polyester, TS , Thermoset Polyester, Mineral Filled
Manufacturer Plenco (Plastics Engineering Company)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 1501 Polyester, Briquette, Transfer Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PLENCO 01501 is a general purpose, mineral filled granular polyester molding compound, offering excellent arc and track resistance properties, low post shrinkage, and improved mechanical strength values. UL recognized under component file E40654. 01501 is available in gray, blue, or tan color.Information supplied by Plenco.
Physical Properties Metric English Comments
Bulk Density 0.750 g/cc
0.0271 lb/in³
ASTM D1895
Density 1.89 g/cc
0.0683 lb/in³
ASTM D792
Water Absorption 0.29 %
0.29 %
ASTM D570
Linear Mold Shrinkage 0.0053 cm/cm
0.0053 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 70
70
ASTM D785
Tensile Strength, Ultimate 51.0 MPa
7400 psi
ASTM D638
Elongation at Break 0.59 %
0.59 %
ASTM D638
Tensile Modulus 11.6 GPa
1680 ksi
ASTM D638
Flexural Strength 92.0 MPa
13300 psi
ASTM D790
Flexural Modulus 11.3 GPa
1640 ksi
ASTM D790
Compressive Strength 161 MPa
23400 psi
ASTM D695
Poissons Ratio 0.32
0.32
ASTM D638
Shear Modulus 4.39 GPa
637 ksi
Calculated
Izod Impact, Notched 0.226 J/cm
0.423 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.254 J/cm²
1.21 ft-lb/in²
ASTM D256
Impact 126
126
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
CTE, linear 54.0 µm/m-°C

@Temperature 40.0 - 130 °C
30.0 µin/in-°F

@Temperature 104 - 266 °F
TMA; ASTM E831
Maximum Service Temperature, Air 171 °C
340 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 208 °C
406 °F
ASTM D648
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
Oxygen Index 24.6 %
24.6 %
ASTM D2863
Shrinkage 0.0167 %
0.0167 %
72 hr, 120ºC; ASTM D1299
Electrical Properties Metric English Comments
Volume Resistivity 2.50e+14 ohm-cm
2.50e+14 ohm-cm
ASTM D247
Dielectric Constant 5.2
5.2
ASTM D150
Dielectric Strength 10.2 kV/mm
259 kV/in
Step by Step; ASTM D149
12.4 kV/mm
315 kV/in
Short Time; ASTM D149
Dielectric Breakdown 14200 V
14200 V
1hr 120C; ASTM D149
Dissipation Factor 0.0278
0.0278
ASTM D150
Arc Resistance 190 sec
190 sec
ASTM D495
Comparative Tracking Index 600 V
600 V
ASTM D3638