Material Notes:
Standard lead-silver-tin eutectic solder with wide application in semiconductor assembly. Often used in reducing atmospheres such as 12% hydrogen. Slightly better corrosion resistance than #101.Information provided by the manufacturer, Indium Corporation.
Physical Properties Metric English Comments
Density 11.28 g/cc
0.4075 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 9.5
9.5
Tensile Strength, Ultimate 30.5 MPa
4420 psi
Elongation at Break 23 %
23 %
Thermal Properties Metric English Comments
CTE, linear 30.0 µm/m-°C

@Temperature 20.0 °C
16.7 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 23.0 W/m-K

@Temperature 85.0 °C
160 BTU-in/hr-ft²-°F

@Temperature 185 °F
Melting Point 309 - 309 °C
588 - 588 °F
Solidus 309 °C
588 °F
Liquidus 309 °C
588 °F
Component Elements Properties Metric English Comments
Lead, Pb 97.5 %
97.5 %
Silver, Ag 1.5 %
1.5 %
Tin, Sn 1.0 %
1.0 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000290 ohm-cm
0.0000290 ohm-cm