Material Notes:
Information Provided by Indium Corporation
Physical Properties Metric English Comments
Density 11.35 g/cc
0.4100 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength at Break 30.5 MPa
4420 psi
Thermal Properties Metric English Comments
CTE, linear 30.0 µm/m-°C

@Temperature 20.0 °C
16.7 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 23.0 W/m-K

@Temperature 85.0 °C
160 BTU-in/hr-ft²-°F

@Temperature 185 °F
Melting Point 304 - 365 °C
579 - 689 °F
Solidus 304 °C
579 °F
Liquidus 365 °C
689 °F
Component Elements Properties Metric English Comments
Lead, Pb 94.5 %
94.5 %
Silver, Ag 5.5 %
5.5 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000290 ohm-cm
0.0000290 ohm-cm
Users viewing this material also viewed the following: