Constellium Formall® 545 Aluminum Alloy

Category Metal , Nonferrous Metal , Aluminum Alloy , 5000 Series Aluminum Alloy
Manufacturer Constellium
Trade Name Formall®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Constellium Formall® 545 Aluminum Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Formall®-545 is a super plastically formable alloy. Both chemical composition and processing conditions have been developed for optimum superplastic behavior and to guarantee the advantages of an aluminum alloy for mechanical construction, i.e.:mechanical strengthgood corrosion resistancefair ability for anodizinggood thermal and electrical conductivitystable in-use propertiesInformation provided by manufacturer
Physical Properties Metric English Comments
Density 2.70 g/cc
0.0975 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength 275 MPa
39900 psi
Temper Delivery condition + 360°C/60'
Tensile Strength, Yield 125 MPa

@Strain 0.200 %
18100 psi

@Strain 0.200 %
Temper Delivery condition + 360°C/60'
Elongation at Break 16 %
16 %
Temper Delivery condition + 360°C/60'
Modulus of Elasticity 71.0 GPa
10300 ksi
Thermal Properties Metric English Comments
CTE, linear 23.8 µm/m-°C

@Temperature 20.0 - 100 °C
13.2 µin/in-°F

@Temperature 68.0 - 212 °F
Thermal Conductivity 105 - 120 W/m-K
729 - 833 BTU-in/hr-ft²-°F
Component Elements Properties Metric English Comments
Aluminum, Al 92.55 - 95.55 %
92.55 - 95.55 %
as balance
Chromium, Cr 0.050 - 0.25 %
0.050 - 0.25 %
Copper, Cu <= 0.10 %
<= 0.10 %
Iron, Fe <= 0.40 %
<= 0.40 %
Magnesium, Mg 4.0 - 4.9 %
4.0 - 4.9 %
Manganese, Mn 0.40 - 1.0 %
0.40 - 1.0 %
Silicon, Si <= 0.40 %
<= 0.40 %
Zinc, Zn <= 0.25 %
<= 0.25 %
Zr+Ti <= 0.15 %
<= 0.15 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000590 - 0.00000660 ohm-cm
0.00000590 - 0.00000660 ohm-cm