Polymer Resources PC-GP4-[color]-6 Polycarbonate, FDA-compliant Feedstocks, Easy Flow with Mold Release

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, Molded
Manufacturer Polymer Resources, LTD
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polymer Resources PC-GP4-[color]-6 Polycarbonate, FDA-compliant Feedstocks, Easy Flow with Mold Release.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polycarbonate, FDA-compliant Feedstocks, Easy Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation.
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ASTM D792
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
ASTM D955
Melt Flow 18 - 30 g/10 min

@Load 1.20 kg,
Temperature 300 °C
18 - 30 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 62.1 MPa
9000 psi
ASTM D638
Tensile Strength, Yield 62.1 MPa
9000 psi
ASTM D638
Flexural Strength 92.4 MPa
13400 psi
ASTM D790
Flexural Modulus 2.28 GPa
330 ksi
ASTM D790
Izod Impact, Notched 6.41 J/cm

@Temperature 22.8 °C
12.0 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Gardner Impact 36.2 J
26.7 ft-lb
ASTM D3029
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 129 °C
265 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 124 °C
255 °F
ASTM D648
Flammability, UL94 V-2

@Thickness 1.70 mm
V-2

@Thickness 0.0669 in
V-2

@Thickness 3.00 mm
V-2

@Thickness 0.118 in
Processing Properties Metric English Comments
Rear Barrel Temperature 249 - 271 °C
480 - 520 °F
Middle Barrel Temperature 260 - 282 °C
500 - 540 °F
Front Barrel Temperature 271 - 293 °C
520 - 560 °F
Melt Temperature 266 - 293 °C
510 - 560 °F
Mold Temperature 65.6 - 93.3 °C
150 - 200 °F
Drying Temperature 118 - 124 °C
245 - 255 °F
Dry Time 3.00 - 4.00 hour
3.00 - 4.00 hour
Descriptive Properties Value Comments
Vent 0.0005