Material Notes:
Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line.
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ASTM D792
Linear Mold Shrinkage 0.0050 cm/cm

@Thickness 3.175 mm
0.0050 in/in

@Thickness 0.1250 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 55.6 MPa
8070 psi
ASTM D638
Elongation at Break 120 %
120 %
ASTM D638
Flexural Strength 82.7 MPa
12000 psi
ASTM D790
Flexural Modulus 2.28 GPa
330 ksi
ASTM D790
Izod Impact, Notched 5.34 J/cm
10.0 ft-lb/in
ASTM D256
Izod Impact, Unnotched NB
NB
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 131 °C
268 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 46.7 °C
116 °F
ASTM D648
Processing Properties Metric English Comments
Melt Temperature 260 - 280 °C
500 - 536 °F
Mold Temperature 65.0 - 95.0 °C
149 - 203 °F
Drying Temperature 110 °C
230 °F
Dry Time 2 - 4 hour
2 - 4 hour
Predrying