Processing Properties | Metric | English | Comments |
---|---|---|---|
Dry Time | 2.00 hour | 2.00 hour | |
PolyOne OnFlex™ S HF 90A-3S1988 Thermoplastic Elastomer (TPE) OnFlex™-S HF thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds utilize a unique, patent pending halogen free flame retardancy system. Fu.. |
|||
Dry Time | 2.00 hour | 2.00 hour | |
PolyOne OnFlex™ S KE 60A-3S1725 Thermoplastic Elastomer (TPE) OnFlex™-S KE thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are specially compatabilized to provide excellent adhesion to a variety p.. |
|||
Dry Time | 2.00 hour | 2.00 hour | |
PolyOne Stat-Tech™ AS-15CF/000 Acrylonitrile Butadiene Styrene (ABS) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Dry Time | 2.00 hour | 2.00 hour | |
PolyOne Edgetek® NY-20CF/000 BLACK Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | |
DuPont Performance Polymers Crastin® S620F20 BK851 PBT
(Unverified Data**) Crastin® S620F20 BK851 is an unreinforced, nucleated, lubricated, medium viscosity, black polybutylene terephthalate resin for fast injection molding.Information provided by DuPont Performance Poly.. |
|||
Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | Injection Molding |
DuPont Performance Polymers Delrin® 100AF Acetal Homopolymer
(Unverified Data**) Delrin® 100AF is a high viscosity acetal homopolymer containing 20% Teflon® PTFE fibers. It is designed for applications requiring low wear and/or low friction against steel, itself, and other pla.. |
|||
Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | |
Pasargad Polymer Peyvand Pasamid 3P-H1130W Nylon 6, 30% Glass Fiber Reinforced Form: PelletsProcessing Method: Injection MoldingUses: Automotive Application Furniture Appliance Components Electrical PartsFastenerHousingInformation provided by Pasargad Polymer Peyvand Co |
|||
Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | Injection Molding |
LG Chemical AF312B ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 79-94-7 and 1309-64-4Information provided by LG Chemical.. |
|||
Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | Injection Molding |
LG Chemical AF345 ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 40039-93-8 and 1309-64-4Information provided by LG Chemi.. |
|||
Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | Injection Molding |
LG Chemical HI121H ABS, High Stiffness Feature: Injection Molding, High StiffnessApplication: Electric & Electronic Products, Miscellaneous GoodsCAS No. 9003-56-9Information provided by LG Chemical |
|||
Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | Injection Molding |
LG Chemical HT700 ABS, High Stiffness Feature: Injection Molding, High StiffnessApplication: Electric & Electronic Products, Miscellaneous GoodsCAS No. 9003-56-9Information provided by LG Chemical |
|||
Dry Time | 2.00 - 3.00 hour | 2.00 - 3.00 hour | Injection Molding |
LG Chemical LUCEL FW700N Modified POM, Friction Resistance, Abrasion Resistance Feature: Injection Molding, Modified POM, Friction Resistance, Abrasion ResistanceApplication: Gears, Printer Roller Pumps, Gear Worm WheelsCAS No. 66455-31-0Information provided by LG Chemical |
|||
Dry Time | 2.00 - 6.00 hour | 2.00 - 6.00 hour | |
Gromax BFM30-EL03N1 Nylon 6 30% Mineral Filled (Conditioned) Information provided by Gromax Enterprises Corp. |
|||
Dry Time | 2.00 - 6.00 hour | 2.00 - 6.00 hour | |
Gromax BFM40-DL04N1 Nylon 6 40% Mineral Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Dry Time | 2.00 - 6.00 hour | 2.00 - 6.00 hour | |
Gromax BTE90-DN001N1 Nylon 6 (Dry) Information provided by Gromax Enterprises Corp. |
|||
Dry Time | 2.00 - 6.00 hour @Temperature 80.0 °C |
2.00 - 6.00 hour @Temperature 176 °F |
|
Lanxess Durethan® BKV 115 H2.0 DUS008 000000 Nylon 6, 15% Glass Fiber PA 6, 15% glass fibers, injection molding, impact modified, heat-ageing stabilizedInformation provided by LANXESS. |
|||
Dry Time | 2.00 - 6.00 hour | 2.00 - 6.00 hour | |
Gromax ATE70-FN00N1 Nylon 6 (Dry) Information provided by Gromax Enterprises Corp. |
|||
Dry Time | 2.00 - 6.00 hour | 2.00 - 6.00 hour | |
Gromax BFG30-DN00N1 Nylon 6 30% Glass Filled (Conditioned) Information provided by Gromax Enterprises Corp. |
|||
Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | |
Lubrizol ESTANE® 58866 Ether Based Thermoplastic Polyurethane Features: Transparent flame retardant compoundUses: Extrusion – Wire and cable, Hose and tubeAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol. |
|||
Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | |
Lubrizol ESTANE® ETE50DS3 Ester Based Thermoplastic Polyurethane Features: Excellent physical and low temperature properties with very good chemical resistance and wide processing window for extrusion.Uses: Flat die/cast film and tubing extrusion and Injection an.. |
|||
Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | Injection Molding |
DuPont Performance Polymers Delrin® 300PE NC010A Acetal Homopolymer Delrin® 300PE NC010A is a medium-high viscosity acetal homopolymer, an enhanced version with extremely low VOC emissions. It has improved processing thermal stability, good mechanical properties, a.. |
|||
Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | DAM; Dehumidified Dryer; Injection Molding |
DuPont Performance Polymers Zytel® ST811HS BK038 Nylon 6
(Unverified Data**) Zytel® ST811HS BK038 is a flexible, non-plasticized, black Super Tough nylon 6 resin developed for extrusion and injection molding applications such as cable and rope jacketing, hose inner cores an.. |
|||
Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | |
Eurotec® Tecomid® NA43 GR25 NL XA43 PA6.6, 25% glass fiber reinforced, flame retardant - red phosphorus free, heat stabilized, natural, UL registered Information provided by Eurotec® |
|||
Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | Handling |
Aremco Corr-Paint™ CP4000-S1 High Temperature Protective Coating, Silicone |
|||
Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | |
Pasargad Polymer Peyvand Pasamid 3P-H2145B Nylon 66, 45% Glass Fiber Reinforced Form: PelletsProcessing Method: Injection MoldingUses: Automotive Application Furniture Appliance Components Electrical PartsFastenerHousingInformation provided by Pasargad Polymer Peyvand Co |
|||
Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | DAM |
DuPont Performance Polymers Zytel® RS 30G30L NC010 Nylon 610
(Unverified Data**) Zytel® RS 30G30L NC010 is a lubricated, 30% glass fiber reinforced polyamide 610 resin containing a minimum of 40% renewably sourced ingredients by weight (60% based on polymer only). It was initia.. |
|||
Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | |
Eurotec® Tecomid® NB40 GR50 NL PA6, 50% glass fiber reinforced, natural Information provided by Eurotec® |
|||
Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | Injection Molding |
DuPont Performance Polymers Delrin® FG311DP NC010 Acetal Homopolymer
(Unverified Data**) Delrin® FG311DP is a medium-high viscosity acetal homopolymer, with improved thermal stability and modifications for more precise molding. It has been developed for consideration into applications .. |
|||
Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | DAM |
DuPont Performance Polymers Zytel® FE5382 BK276 Nylon 612
(Unverified Data**) Zytel® FE5382 BK276 is a 33% glass fiber reinforced, heat stabilized, black polyamide 612 resin developed for electrical bobbins and encapsulation applications.Information provided by DuPont Perfor.. |