Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lubrizol ESTANE® ETE50DS3 Ester Based Thermoplastic Polyurethane

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP , Thermoplastic Polyurethane, Elastomer, Polyester Grade
Manufacturer Lubrizol (former Noveon)
Trade Name ESTANE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol ESTANE® ETE50DS3 Ester Based Thermoplastic Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: Excellent physical and low temperature properties with very good chemical resistance and wide processing window for extrusion.Uses: Flat die/cast film and tubing extrusion and Injection and blow molding.Available in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol.
Physical Properties Metric English Comments
Specific Gravity 1.22 g/cc
1.22 g/cc
ASTM D792
Maximum Moisture Content 0.020
0.020
Mechanical Properties Metric English Comments
Hardness, Shore D 49

@Time 5.00 sec
49

@Time 0.00139 hour
ASTM D2240
Tensile Strength 65.5 MPa
9500 psi
ASTM D412
65.5 MPa

@Temperature 23.0 °C,
Time 0.000 sec
9500 psi

@Temperature 73.4 °F,
Time 0.000 hour
Sheet Immersion in Diesel Fuel
65.5 MPa

@Temperature 23.0 °C,
Time 2.42e+6 sec
9500 psi

@Temperature 73.4 °F,
Time 672 hour
Sheet Immersion in Diesel Fuel
72.05 MPa

@Temperature 23.0 °C,
Time 1.30e+6 sec
10450 psi

@Temperature 73.4 °F,
Time 360 hour
Sheet Immersion in Diesel Fuel
Elongation at Break 440 %
440 %
ASTM D412
100% Modulus 0.0104 GPa
1.51 ksi
ASTM D412
300% Modulus 0.0310 GPa
4.50 ksi
ASTM D412
Flexural Stiffness 112.00 MPa
16244 psi
Tear Strength 33.3 kN/m
190 pli
Trouser; ASTM D470
Graves Tear Strength 131 kN/m
750 pli
Die C; ASTM D624
Taber Abrasion, mg/1000 Cycles 50
50
H18, 1000g; ASTM D3389 B
Tensile Set 22 %
22 %
200% elongation; ASTM D412
Thermal Properties Metric English Comments
Melting Point 176 °C
349 °F
Kofler
177 °C
351 °F
DSC
Glass Transition Temp, Tg -36.0 °C
-32.8 °F
DSC
Processing Properties Metric English Comments
Zone 1 182 °C
360 °F
Extrusion
Zone 2 188 °C
370 °F
Extrusion
Zone 3 193 °C
379 °F
Extrusion
Zone 4 199 °C
390 °F
Extrusion
Adapter Temperature 204 °C
399 °F
5, Extrusion
Die Temperature 204 °C
399 °F
Zone 1, Extrusion
204 °C
399 °F
Zone 2, Extrusion
Drying Temperature 104 °C
219 °F
Dry Time 2.00 - 4.00 hour
2.00 - 4.00 hour
Dew Point -40.0 °C
-40.0 °F
Descriptive Properties Value Comments
Volume swell in Diesel Fuel 6.1%
24h, 23°C; ASTM D471