Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Beijing Chemical Industry KAIFA® MN301-G20 Nylon 66 Resin

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Glass Fiber Filled, Flame Retardant
Manufacturer Beijing Chemical Industry Research Institute (Group)
Trade Name KAIFA®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Beijing Chemical Industry KAIFA® MN301-G20 Nylon 66 Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
20% glass fiber reinforced, flame retardantInformation provided by Beijing Chemical Industry Research Institute (Group)
Physical Properties Metric English Comments
Density 1.48 g/cc
0.0535 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0040 - 0.0080 cm/cm
0.0040 - 0.0080 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 110 MPa
16000 psi
ASTM D638
Flexural Strength 155 MPa
22500 psi
ASTM D790
Charpy Impact Unnotched 5.60 J/cm²
26.7 ft-lb/in²
ISO179
Charpy Impact, Notched 1.00 J/cm²
4.76 ft-lb/in²
ISO179
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 235 °C
455 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 3.20 mm
V-0

@Thickness 0.126 in
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
ASTM D257
Dielectric Constant 3.2

@Frequency 1e+6 Hz
3.2

@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 28.0 kV/mm

@Thickness 2.00 mm
711 kV/in

@Thickness 0.0787 in
ASTM D149
Dissipation Factor 0.017

@Frequency 1e+6 Hz
0.017

@Frequency 1e+6 Hz
ASTM D150
Processing Properties Metric English Comments
Rear Barrel Temperature 230 - 240 °C
446 - 464 °F
Middle Barrel Temperature 265 - 270 °C
509 - 518 °F
Front Barrel Temperature 265 - 270 °C
509 - 518 °F
Nozzle Temperature 265 - 270 °C
509 - 518 °F
Mold Temperature 60.0 - 90.0 °C
140 - 194 °F
Drying Temperature 130 °C
266 °F
Dry Time 4 hour
4 hour
Injection Pressure 90.0 - 120 MPa
13100 - 17400 psi
Users viewing this material also viewed the following: