Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 43.3 °C | 110 °F | |
Northstar Polymers MSB-M25B Microcellular Foam based on High Performance Polyester Polyurethane This high performance polyester microcellular foam system is one of a family of polymer systems developed by Northstar Polymers for demanding work environments. Urethane foams molded with this syste.. |
|||
Mold Temperature | 43.3 - 82.2 °C | 110 - 180 °F | |
Polymer Resources TP-FR IM PBT, Impact Modified, Flame Retardant, Low Flow Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Mold Temperature | 43.3 - 60.0 °C | 110 - 140 °F | |
Polymer Resources TP-FR2 Polybutylene Terephthalate, Flame Retardant Polybutylene Terephthalate, Flame Retardant Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided.. |
|||
Mold Temperature | 43.3 - 82.2 °C | 110 - 180 °F | |
Polymer Resources TP-FR-IM Polybutylene Terephthalate, Impact Modified, Flame Retardant, Low Flow Polybutylene Terephthalate, Impact Modified, Flame Retardant, Low FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sa.. |
|||
Mold Temperature | 43.3 - 76.7 °C | 110 - 170 °F | |
Polymer Resources TP-GP1F Polybutylene Terephthalate, General Purpose, FDA-compliant Feedstocks Polybutylene Terephthalate, General Purpose, FDA-compliant FeedstocksProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sam.. |
|||
Mold Temperature | 43.3 - 76.7 °C | 110 - 170 °F | |
Polymer Resources TP-GP1-IM Polybutylene Terephthalate, Impact Modified, Medium Flow Polybutylene Terephthalate, Impact Modified, Medium FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informat.. |
|||
Mold Temperature | 43.3 - 76.7 °C | 110 - 170 °F | |
Polymer Resources TP-IM1 Polybutylene Terephthalate, Low Temperature Impact Modified Polybutylene Terephthalate, Low Temperature Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor.. |
|||
Mold Temperature | 43.3 - 90.0 °C | 110 - 194 °F | Average value: 65.2 °C Grade Count:5 |
Overview of materials for Acrylic, Heat Resistant, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Heat Resistant, Molded". Each property range of values reported is minimum and maximum values o.. |
|||
Mold Temperature | 43.3 - 65.6 °C | 110 - 150 °F | |
Calsak CS-72 General Purpose ABS Resin Product Characteristics:High Impact, High GlossInjection molding grade |
|||
Mold Temperature | 43.3 - 65.6 °C | 110 - 150 °F | |
Calsak CS-72L General Purpose ABS Resin Product Characteristics:High Impact, High GlossInjection molding grade |
|||
Mold Temperature | 43.3 - 54.4 °C | 110 - 130 °F | |
Advanced Polymer Alloys DuraGrip™ 6150 BK Melt Processable Elastomer DuraGrip™ 6150BK is designed to be a special purpose Melt Processable Elastomer (MPE) that is easy to use in injection molding and extrusion processes. DGR 6150BK has an excellent
soft touch feel a.. |
|||
Mold Temperature | 43.3 - 54.4 °C | 110 - 130 °F | |
Advanced Polymer Alloys DuraGrip™ 6160 BK Melt Processable Elastomer DuraGrip™ 6160BK is designed to be a special purpose Melt Processable Elastomer (MPE) that is easy to use in injection molding and extrusion processes. DGR 6160BK has an excellent
soft touch feel a.. |
|||
Mold Temperature | 43.3 - 54.4 °C | 110 - 130 °F | |
Advanced Polymer Alloys DuraGrip™ DGR 6030 NC/BK Thermoplastic Elastomer (TPE) DuraGrip® DGR 6030 NC/BK are designed to be general purpose Thermoplastic Elastomers (TPE) that are easy to use in injection molding and extrusion processes. DGR 6030 NC/BK have
an excellent soft t.. |
|||
Mold Temperature | 43.3 - 54.4 °C | 110 - 130 °F | |
Advanced Polymer Alloys DuraGrip™ DGR 6040 NC/BK Thermoplastic Elastomer (TPE) DuraGrip® DGR 6040 NC/BK are designed to be general purpose Thermoplastic Elastomers (TPE) that are easy to use in injection molding and extrusion processes. DGR 6040 NC/BK have
an excellent soft t.. |
|||
Mold Temperature | 43.3 - 54.4 °C | 110 - 130 °F | |
Advanced Polymer Alloys DuraGrip™ DGR 6050 NC/BK Thermoplastic Elastomer (TPE) DuraGrip® DGR 6050 NC/BK are designed to be general purpose Thermoplastic Elastomers (TPE) that are easy to use in injection molding and extrusion processes. DGR 6050 NC/BK have
an excellent soft t.. |
|||
Mold Temperature | 43.3 - 54.4 °C | 110 - 130 °F | |
Advanced Polymer Alloys DuraGrip™ DGR 6070 NC Thermoplastic Elastomer (TPE) DuraGrip® DGR 6070NC is designed to be a general purpose Thermoplastic Elastomer (TPE) that is easy to use in injection molding and extrusion processes. DGR 6070NC has an
excellent soft touch feel,.. |
|||
Mold Temperature | 43.3 - 54.4 °C | 110 - 130 °F | |
Advanced Polymer Alloys DuraGrip™ DGR 6080 NC/BK Thermoplastic Elastomer (TPE) DuraGrip® DGR 6080NC/BK are designed to be a general purpose Thermoplastic Elastomers (TPE) that are easy to use in injection molding and extrusion processes. DGR
6080NC/BK have excellent soft touc.. |
|||
Mold Temperature | 43.3 - 51.7 °C | 110 - 125 °F | |
LNP Thermocomp® HF-1006 Polyamide 11, Glass Fiber Reinforcement
(discontinued **) Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names.. |