Material Notes:
Zytel® 7335F NC010 is a nucleated, lubricated polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
DAM; ISO 1183
Water Absorption 3.0 %

@Temperature 23.0 °C
3.0 %

@Temperature 73.4 °F
Equilibrium 50%RH; DAM; ISO 62, Similar to
9.0 %

@Temperature 23.0 °C
9.0 %

@Temperature 73.4 °F
Saturation, immersed; DAM; ISO 62, Similar to
Linear Mold Shrinkage 0.0075 cm/cm

@Thickness 1.60 mm
0.0075 in/in

@Thickness 0.0630 in
DAM
0.010 cm/cm

@Thickness 3.20 mm
0.010 in/in

@Thickness 0.126 in
DAM
Linear Mold Shrinkage, Flow 0.0060 cm/cm

@Thickness 2.00 mm
0.0060 in/in

@Thickness 0.0787 in
DAM; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0080 cm/cm

@Thickness 2.00 mm
0.0080 in/in

@Thickness 0.0787 in
DAM; ISO 294-4
Mechanical Properties Metric English Comments
Tensile Strength, Yield 55.0 MPa

@Temperature 23.0 °C
7980 psi

@Temperature 73.4 °F
50%RH; ISO 527
90.0 MPa

@Temperature 23.0 °C
13100 psi

@Temperature 73.4 °F
DAM; ISO 527
Elongation at Break 9.0 %

@Temperature 23.0 °C
9.0 %

@Temperature 73.4 °F
DAM; nominal; ISO 527
15 %

@Temperature 23.0 °C
15 %

@Temperature 73.4 °F
50mm/min; DAM; ISO 527
>= 50 %

@Temperature 23.0 °C
>= 50 %

@Temperature 73.4 °F
50mm/min; 50%RH; ISO 527
>= 50 %

@Temperature 23.0 °C
>= 50 %

@Temperature 73.4 °F
50%RH; nominal; ISO 527
Elongation at Yield 3.8 %

@Temperature 23.0 °C
3.8 %

@Temperature 73.4 °F
DAM; ISO 527
24 %

@Temperature 23.0 °C
24 %

@Temperature 73.4 °F
50%RH; ISO 527
Tensile Modulus 1.40 GPa

@Temperature 23.0 °C
203 ksi

@Temperature 73.4 °F
50%RH; ISO 527
3.60 GPa

@Temperature 23.0 °C
522 ksi

@Temperature 73.4 °F
DAM; ISO 527
Charpy Impact Unnotched 6.00 J/cm²

@Temperature -30.0 °C
28.6 ft-lb/in²

@Temperature -22.0 °F
50%RH; ISO 179/1eU
7.00 J/cm²

@Temperature 23.0 °C
33.3 ft-lb/in²

@Temperature 73.4 °F
DAM; ISO 179/1eU
11.0 J/cm²

@Temperature -30.0 °C
52.3 ft-lb/in²

@Temperature -22.0 °F
DAM; ISO 179/1eU
12.0 J/cm²

@Temperature 23.0 °C
57.1 ft-lb/in²

@Temperature 73.4 °F
50%RH; ISO 179/1eU
Charpy Impact, Notched 0.250 J/cm²

@Temperature -30.0 °C
1.19 ft-lb/in²

@Temperature -22.0 °F
DAM; ISO 179/1eA
0.300 J/cm²

@Temperature -30.0 °C
1.43 ft-lb/in²

@Temperature -22.0 °F
50%RH; ISO 179/1eA
0.450 J/cm²

@Temperature 23.0 °C
2.14 ft-lb/in²

@Temperature 73.4 °F
DAM; ISO 179/1eA
1.80 J/cm²

@Temperature 23.0 °C
8.57 ft-lb/in²

@Temperature 73.4 °F
50%RH; ISO 179/1eA
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 500 µm/m-°C

@Temperature 23.0 - 55.0 °C
278 µin/in-°F

@Temperature 73.4 - 131 °F
DAM; ASTM E 831
500 µm/m-°C

@Temperature 23.0 - 55.0 °C
278 µin/in-°F

@Temperature 73.4 - 131 °F
DAM; ISO 11359-1/-2
CTE, linear, Transverse to Flow 92.0 µm/m-°C

@Temperature 23.0 - 55.0 °C
51.1 µin/in-°F

@Temperature 73.4 - 131 °F
DAM; ASTM E 831
92.0 µm/m-°C

@Temperature 23.0 - 55.0 °C
51.1 µin/in-°F

@Temperature 73.4 - 131 °F
DAM; ISO 11359-1/-2
Melting Point 221 °C
430 °F
10°C/min; DAM; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 175 °C
347 °F
DAM; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °C
149 °F
DAM; ISO 75-1/-2
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
DAM; UL94
HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
DAM; IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+11 ohm-cm

@Temperature 23.0 °C
1.00e+11 ohm-cm

@Temperature 73.4 °F
50%RH; ASTM D257
1.00e+11 ohm-cm

@Temperature 23.0 °C
1.00e+11 ohm-cm

@Temperature 73.4 °F
50%RH; IEC 60093
>= 1.00e+15 ohm-cm

@Temperature 23.0 °C
>= 1.00e+15 ohm-cm

@Temperature 73.4 °F
DAM; IEC 60093
1.00e+17 ohm-cm

@Temperature 23.0 °C
1.00e+17 ohm-cm

@Temperature 73.4 °F
DAM; ASTM D257
1.00e+17 ohm-cm

@Temperature 23.0 °C
1.00e+17 ohm-cm

@Temperature 73.4 °F
DAM; IEC 60093
Surface Resistance 1.00e+11 ohm

@Temperature 23.0 °C
1.00e+11 ohm

@Temperature 73.4 °F
50%RH; ASTM D257
1.00e+11 ohm

@Temperature 23.0 °C
1.00e+11 ohm

@Temperature 73.4 °F
50%RH; IEC 60093
1.00e+13 ohm

@Temperature 23.0 °C
1.00e+13 ohm

@Temperature 73.4 °F
DAM; ASTM D257
Dielectric Constant 3.3

@Frequency 1.00e+6 Hz,
Temperature 23.0 °C
3.3

@Frequency 1.00e+6 Hz,
Temperature 73.4 °F
DAM; ASTM D150
3.6

@Frequency 100 Hz,
Temperature 23.0 °C
3.6

@Frequency 100 Hz,
Temperature 73.4 °F
DAM; ASTM D150
3.6

@Frequency 1000 Hz,
Temperature 23.0 °C
3.6

@Frequency 1000 Hz,
Temperature 73.4 °F
DAM; ASTM D150
4.2

@Frequency 100 Hz,
Temperature 23.0 °C
4.2

@Frequency 100 Hz,
Temperature 73.4 °F
DAM; IEC 60250
Dielectric Strength 13.5 kV/mm

@Thickness 3.20 mm,
Temperature 23.0 °C
343 kV/in

@Thickness 0.126 in,
Temperature 73.4 °F
50%RH; Short Time; ASTM D149
16.3 kV/mm

@Thickness 3.20 mm,
Temperature 23.0 °C
414 kV/in

@Thickness 0.126 in,
Temperature 73.4 °F
DAM; Short Time; ASTM D149
Dissipation Factor 0.010

@Frequency 1000 Hz,
Temperature 23.0 °C
0.010

@Frequency 1000 Hz,
Temperature 73.4 °F
DAM; ASTM D150
0.010

@Frequency 100 Hz,
Temperature 23.0 °C
0.010

@Frequency 100 Hz,
Temperature 73.4 °F
DAM; ASTM D150
0.020

@Frequency 1.00e+6 Hz,
Temperature 23.0 °C
0.020

@Frequency 1.00e+6 Hz,
Temperature 73.4 °F
DAM; ASTM D150
0.030

@Frequency 100 Hz,
Temperature 23.0 °C
0.030

@Frequency 100 Hz,
Temperature 73.4 °F
DAM; IEC 60250
0.11

@Frequency 1.00e+6 Hz,
Temperature 23.0 °C
0.11

@Frequency 1.00e+6 Hz,
Temperature 73.4 °F
50%RH; ASTM D150
0.23

@Frequency 1000 Hz,
Temperature 23.0 °C
0.23

@Frequency 1000 Hz,
Temperature 73.4 °F
50%RH; ASTM D150
0.37

@Frequency 100 Hz,
Temperature 23.0 °C
0.37

@Frequency 100 Hz,
Temperature 73.4 °F
50%RH; ASTM D150
Comparative Tracking Index 600 V

@Temperature 23.0 °C
600 V

@Temperature 73.4 °F
DAM; IEC 60112
Processing Properties Metric English Comments
Melt Temperature 260 - 280 °C
500 - 536 °F
DAM
270 °C
518 °F
DAM; Optimum
Mold Temperature 70.0 °C
158 °F
DAM; optimum
50.0 - 90.0 °C
122 - 194 °F
DAM
Drying Temperature 80.0 °C
176 °F
DAM
Dry Time 2.00 - 4.00 hour
2.00 - 4.00 hour
DAM
Moisture Content <= 0.20 %
<= 0.20 %
DAM
Descriptive Properties Value Comments
Additive Lubricant
DAM
Appearance Natural Color
DAM
Drying Recommended Yes, if moisture content of resin exceeds recommended level
DAM
Features Chemical Resistance, Good
DAM
Fatigue Resistant
DAM
Fuel Resistant
DAM
General Purpose
DAM
Grease Resistant
DAM
Mold Release, Good
DAM
Nucleated
DAM
Oil Resistant
DAM
Forms Pellets
DAM
Generic Nylon 6
DAM
Material Status Current
DAM
Part Marking Code >PA6<
ISO 11469; DAM
Polymer Family Polyamide
DAM
Polymer Type PA6
DAM
Processing Method Injection Molding
DAM
Product Category Unreinforced Resins
DAM
Resin Identification PA6
ISO 1043; DAM
RoHS Compliance Contact Manufacturer
DAM
Ultrasonic Weldable Yes
DAM
Uses Appliance Components
DAM
Automotive Applications
DAM
Electrical/Electronic Applications
DAM
Users viewing this material also viewed the following: