Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Eurostar Staramide 6 80E7 PA6, Injection Molded

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer Eurostar Engineering Plastics
Trade Name Staramide
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eurostar Staramide 6 80E7 PA6, Injection Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Staramide 6 80E7 is a high density, Polyamide 6, Injection Molding Resin (also known as 680E7)Information provided by Eurostar.
Physical Properties Metric English Comments
Density 2.99 g/cc
0.108 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0070 - 0.010 cm/cm

@Thickness 4.00 mm
0.0070 - 0.010 in/in

@Thickness 0.157 in
E2P method
Mechanical Properties Metric English Comments
Tensile Strength at Break 74.0 MPa
10700 psi
ISO 527
Elongation at Break 0.90 %
0.90 %
ISO 527
Flexural Strength 102 MPa
14800 psi
ISO 178
Flexural Modulus 9.50 GPa
1380 ksi
ISO 178
Izod Impact, Notched (ISO) 4.00 kJ/m²
1.90 ft-lb/in²
80x10x4; ISO 180/1A
Izod Impact, Unnotched (ISO) 17.0 kJ/m²
8.09 ft-lb/in²
80x10x4; ISO 180/1U
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 132 °C
270 °F
Flatw 80x10x4, sp=64 mm; ISO 75/Af
Processing Properties Metric English Comments
Zone 1 250 - 260 °C
482 - 500 °F
Zone 2 260 - 280 °C
500 - 536 °F
Zone 3 260 - 280 °C
500 - 536 °F
Melt Temperature 260 - 280 °C
500 - 536 °F
Mold Temperature 50.0 - 90.0 °C
122 - 194 °F
Drying Temperature 80.0 °C

@Time 14400 sec
176 °F

@Time 4.00 hour
Moisture Content 0.20 %
0.20 %