Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Performance Polymers Delrin® 300TE BK602 Acetal Homopolymer  (Unverified Data**)

Category Polymer , Thermoplastic , Acetal (POM)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Delrin® 300TE BK602 Acetal Homopolymer  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Delrin® 300TE BK602 is a medium-high viscosity toughened acetal homopolymer for injection molding with extremely low VOC emissions.Information provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Density 1.38 g/cc
0.0499 lb/in³
ISO 1183
Melt Flow 6.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
6.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 54.0 MPa

@Temperature 23.0 °C
7830 psi

@Temperature 73.4 °F
ISO 527
Elongation at Break 33 %

@Temperature 23.0 °C
33 %

@Temperature 73.4 °F
nominal; ISO 527
Elongation at Yield 20 %

@Temperature 23.0 °C
20 %

@Temperature 73.4 °F
ISO 527
Tensile Modulus 1.90 GPa

@Temperature 23.0 °C
276 ksi

@Temperature 73.4 °F
ISO 527
Charpy Impact, Notched 1.00 J/cm²

@Temperature -30.0 °C
4.76 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
1.80 J/cm²

@Temperature 23.0 °C
8.57 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 178 °C
352 °F
10°C/min; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 72.0 °C
162 °F
ISO 75-1/-2
Processing Properties Metric English Comments
Melt Temperature 205 °C
401 °F
Optimum; Injection Molding
200 - 210 °C
392 - 410 °F
Injection Molding
Mold Temperature 50.0 °C
122 °F
optimum; Injection Molding
40.0 - 60.0 °C
104 - 140 °F
Injection Molding
Drying Temperature 80.0 °C
176 °F
Dry Time 2.00 - 4.00 hour
2.00 - 4.00 hour
Moisture Content <= 0.050 %
<= 0.050 %
Descriptive Properties Value Comments
Forms Pellets
Generic Acetal (POM) Homopolymer
Material Status Preliminary Data
Part Marking Code >POM-I<
ISO 11469
Processing Method Injection Molding
Product Category Low Emissions Resins
Toughened Resins
Region Available - Global Yes
Resin Identification POM-I
ISO 1043
RoHS Compliance Contact Manufacturer