Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

NHEP Spectron™ E6666 Nylon 66, 30% Glass Fiber

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Glass Fiber Filled
Manufacturer Ngai Hing Hong Engineering Plastic (Hong Kong) Ltd .
Trade Name Spectron™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NHEP Spectron™ E6666 Nylon 66, 30% Glass Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Natural color. E6666 exhibits high rigidity, mechanical strength, and excellent appearance. It is suitable for wide range of applications.Property data measured at room temperature, 50% RH.Information provided by Bieglo Gmbh for Ngai Hing Engineering Plastic (Hong Kong) Ltd.
Physical Properties Metric English Comments
Density 1.37 g/cc
0.0495 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm
0.0040 - 0.0070 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength 165 MPa
23900 psi
ASTM D638
Elongation at Yield 7.0 %
7.0 %
ASTM D638
Flexural Strength 220 MPa
31900 psi
ASTM D790
Flexural Modulus 8.40 GPa
1220 ksi
ASTM D790
Izod Impact, Notched 0.800 J/cm
1.50 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 240 °C
464 °F
ASTM D648
Processing Properties Metric English Comments
Rear Barrel Temperature 260 - 270 °C
500 - 518 °F
Middle Barrel Temperature 260 - 270 °C
500 - 518 °F
Front Barrel Temperature 260 - 270 °C
500 - 518 °F
Nozzle Temperature 270 - 280 °C
518 - 536 °F
Mold Temperature 100 - 120 °C
212 - 248 °F
Drying Temperature 100 - 120 °C

@Time 7200 - 14400 sec
212 - 248 °F

@Time 2.00 - 4.00 hour
Descriptive Properties Value Comments
Processing Injection Pressure Medium-High
Processing Injection Speed Medium-High