Material Notes:
Dissipative product based on Polycarbonate (PC). Unfilled. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.A.
Physical Properties Metric English Comments
Density 1.22 g/cc
0.0441 lb/in³
Linear Mold Shrinkage, Flow 0.0070 - 0.0090 cm/cm
0.0070 - 0.0090 in/in
Linear Mold Shrinkage, Transverse 0.0070 - 0.0090 cm/cm
0.0070 - 0.0090 in/in
Mechanical Properties Metric English Comments
Tensile Strength at Break 50.0 MPa
7250 psi
Elongation at Yield 4.5 %
4.5 %
Tensile Modulus 2.60 GPa
377 ksi
Charpy Impact Unnotched 9.50 J/cm²
45.2 ft-lb/in²
Charpy Impact, Notched 2.00 J/cm²
9.52 ft-lb/in²
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 120 °C
248 °F
Deflection Temperature at 0.46 MPa (66 psi) 135 °C
275 °F
Deflection Temperature at 1.8 MPa (264 psi) 125 °C
257 °F
Vicat Softening Point 145 °C

@Load 5.00 kg
293 °F

@Load 11.0 lb
Electrical Properties Metric English Comments
Surface Resistance 10000 ohm
10000 ohm
Processing Properties Metric English Comments
Melt Temperature 270 - 290 °C
518 - 554 °F
Mold Temperature 100 - 120 °C
212 - 248 °F
Drying Temperature 120 - 130 °C

@Time 10800 sec
248 - 266 °F

@Time 3.00 hour
Descriptive Properties Value Comments
ISO Shrinkage - Pressure 60 MPa