Processing Properties Metric English Comments
Nozzle Temperature 190 - 215 °C
374 - 419 °F
PTS POM-270 27.0 MFI Acetal Copolymer
Information provided by Polymer Technology and Services, LLC (PTS).
Nozzle Temperature 190 - 215 °C
374 - 419 °F
PTS POM-90 9.0 MFI Acetal Copolymer
Information provided by Polymer Technology and Services, LLC (PTS).
Nozzle Temperature 200 - 215 °C
392 - 419 °F
Extrusion
Huntsman IROGRAN® A 95 E 4861 Polyester-Based TPU-Injection Extrusion Grade
Introduction: IROGRAN A95 4861 is a high performance polyester based thermoplastic polyurethane intended for extrusion applications. IROGRAN A95E 4861 is part of the HUNTSMAN technical extrusion pro..
Nozzle Temperature 195 - 215 °C
383 - 419 °F
Injection Molding
LG Chemical KEYFLEX BT 1030D Ester Type TPE
Description: Injection Molding, TPC-ET, General Purpose, Low ModulusApplication: Automotive Interior, Soft Touch GripsCAS: 37282-12-5Information provided by LG Chemical
Nozzle Temperature 190 - 215 °C
374 - 419 °F
LG Chemical Lucet® N109 Acetal Copolymer
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Nozzle Temperature 190 - 215 °C
374 - 419 °F
LG Chemical Lucet® N127 Acetal Copolymer
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Nozzle Temperature 200 - 215 °C
392 - 419 °F
Injection Molding
Ineos ABS Lustran® SAN DN59 SAN, Soft-Flow Grade
Lustran® SAN DN59 resin is a soft-flow grade of transparent SAN (styrene acrylonitrile) thermoplastic. It has been designed for use in compounding and thin-wall injection molded applications. Lus..
Nozzle Temperature 205 - 215 °C
401 - 419 °F
Lubrizol Advanced Materials Pearlthane® ECO D12T90 Thermoplastic Polyurethane
Type : Pearlthane® ECO D12T90 is a high performance bio-based thermoplastic polyurethane. With ca. 38% bio-based content.Main Application : Injection MouldingSpecial Features : Very good flexibil..
Nozzle Temperature 205 - 215 °C
401 - 419 °F
Huntsman AVALON® 90 AK Thermoplastic Polyurethane
Introduction: AVALON 90 AK is a part of the AVALON Crystal Range and offers a specially designed, flexible material wit a higher degree of transparency compared with conventional TPU at the same har..
Nozzle Temperature 205 - 215 °C
401 - 419 °F
Huntsman AVALON® 90 AKU Thermoplastic Polyurethane
Introduction: AVALON 90 AKU is a part of the AVALON Crystal Range and offers a specially designed, flexible material wit a higher degree of transparency compared with conventional TPU at the same ha..
Nozzle Temperature 200 - 215 °C
392 - 419 °F
Lubrizol Estane® S195A Thermoplastic Polyurethane
Type: Estane® S195A is a Shore 95A, polyester based thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding.Availability: Americas, Europe, Middle East, ..
Nozzle Temperature 200 - 215 °C
392 - 419 °F
Lubrizol Estane® S198A Thermoplastic Polyurethane
Type: Estane® S198A is a Shore 98A, polyester grade thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding.Availability: Americas, Europe, Middle East, ..
Nozzle Temperature 205 - 215 °C
401 - 419 °F
Injection
Lubrizol ESTANE® GP52DB Ester Based Thermoplastic Polyurethane
Type: Estane® GP 52DB is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b..
Nozzle Temperature 205 - 215 °C
401 - 419 °F
Injection
Lubrizol ESTANE® GP60DE Ester Based Thermoplastic Polyurethane
Estane® GP 60DE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided by Lubr..
Nozzle Temperature 200 - 215 °C
392 - 419 °F
Lubrizol Estane® L194A Thermoplastic Polyurethane
Type: Estane® L194A is a Shore 95A, polyester grade thermoplastic polyurethane (TPU).Uses: Injection Molding.Availability: AsiaInformation Provided by The Lubrizol Corporation
Nozzle Temperature 205 - 215 °C
401 - 419 °F
Injection
Alliance Polymers Zythane™ 4045D Thermoplastic Polyurethane Elastomer
Zythane™ 4045D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Nozzle Temperature 200 - 215 °C
392 - 419 °F
Injection
Alliance Polymers Zythane™ 4085A Thermoplastic Polyurethane Elastomer
Zythane™ 4085A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Nozzle Temperature 205 - 215 °C
401 - 419 °F
Injection
Alliance Polymers Zythane™ 4090A Thermoplastic Polyurethane Elastomer
Zythane™ 4090A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Nozzle Temperature 205 - 215 °C
401 - 419 °F
Injection
Alliance Polymers Zythane™ 5045D Thermoplastic Polyurethane Elastomer
Zythane™ 5045D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Nozzle Temperature 205 - 215 °C
401 - 419 °F
Injection
Alliance Polymers Zythane™ 6045D Thermoplastic Polyurethane Elastomer
Zythane™ 6045D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Nozzle Temperature 205 - 215 °C
401 - 419 °F
Injection
Alliance Polymers Zythane™ 6090A Thermoplastic Polyurethane Elastomer
Zythane™ 6090A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Nozzle Temperature 205 - 215 °C
401 - 419 °F
Injection
Alliance Polymers Zythane™ 7045A Thermoplastic Polyurethane Elastomer
Zythane™ 7045A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Nozzle Temperature 200 - 215 °C
392 - 419 °F
Injection
Alliance Polymers Zythane™ 7085A Thermoplastic Polyurethane Elastomer
Zythane™ 7085A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Nozzle Temperature 205 - 215 °C
401 - 419 °F
Injection
Alliance Polymers Zythane™ 7085AF Thermoplastic Polyurethane Elastomer
Zythane™ 7085AF is a FR polyether-based TPU specifically formulated with non-halogenated flame retardants for extrusion applications with ease of processing. It exhibits excellent abrasion resistan..
Nozzle Temperature 200 - 215 °C
392 - 419 °F
Celanese Riteflex® 647 Thermoplastic Polyester Elastomer (TPE)
Description: Riteflex 647 is a thermoplastic elastomer with a 47 Shore D hardness and a 21,300psi flexural modulusInformation provided by Celanese Corporation.
Nozzle Temperature 195 - 215 °C
383 - 419 °F
Celanese Vandar® 9118 Unfilled Polyester Alloy
Description: Vandar 9118 is an unfilled polyester alloy which exhibits excellent toughness and impact strength. It is typically used for unpainted cover/container applicationsInformation provided by..
Nozzle Temperature 195 - 215 °C
383 - 419 °F
Celanese Vandar® AB200 Low Modulus Polyester Alloy
Description: Vandar AB200 is a low modulus polyester alloy which exhibits excellent toughness and impact strength. It is typically used for driver airbag covers.Information provided by Celanese Corp..
Nozzle Temperature 200 - 215 °C
392 - 419 °F
Injection
Alliance Polymers Zythane™ 5085A Thermoplastic Polyurethane Elastomer
Zythane™ 5085A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Nozzle Temperature 200 - 215 °C
392 - 419 °F
Injection
Alliance Polymers Zythane™ 7085AU Thermoplastic Polyurethane Elastomer
Zythane™ 7085UF is a UV stabilized polyether-based TPU specifically formulated for extrusion applications. It exhibits excellent abrasion resistance and toughness and has good hydrolytic stability,..
Nozzle Temperature 205 - 215 °C
401 - 419 °F
Injection
Lubrizol Estane® GP 52 DT Thermoplastic Polyurethane
Type: Estane® GP 52DT is an aromatic polyester-based thermoplastic polyurethane (TPU).Features: Translucent spherical pellets.Uses: Injection molding parts, animal identification tagsAvailable in E..
Copyright © lookpolymers.com All Rights Reserved