Lubrizol Advanced Materials PEARLTHANE® 11T80 Thermoplastic Polyurethane Elastomer

Category Polymer , Thermoplastic , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyester Grade
Manufacturer Lubrizol Advanced Materials Manufacturing S. S.L. (Former Merquinsa)
Trade Name Pearlthane®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol Advanced Materials PEARLTHANE® 11T80 Thermoplastic Polyurethane Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Type : Pearlthane® 11T80 is a polycaprolactone copolyester-based thermoplastic polyurethane.Main Application : Injection MouldingSpecial Features : Combining hardness with excellent mechanical properties as well as an improved transparancy. All information provided by Merquinsa
Physical Properties Metric English Comments
Specific Gravity 1.16 g/cc
1.16 g/cc
ISO 2781
Mechanical Properties Metric English Comments
Hardness, Shore A 82
82
ISO 868
Tensile Strength 40.00 MPa
5801 psi
ISO 527-2/5A/500
Elongation at Break 630 %
630 %
ISO 527-2/5A/500
50% Modulus 0.00400 GPa
0.580 ksi
ISO 527-2/5A/500
100% Modulus 0.00500 GPa
0.725 ksi
ISO 527-2/5A/500
300% Modulus 0.00800 GPa
1.16 ksi
ISO 527-2/5A/500
Tear Strength 79.8 kN/m
455 pli
ISO 34-1B
Abrasion 20
20
loss (mm³); ISO 4649-A
Thermal Properties Metric English Comments
Vicat Softening Point 77.0 °C
171 °F
ISO 306
Processing Properties Metric English Comments
Feed Temperature 40.0 °C
104 °F
Nozzle Temperature 185 - 215 °C
365 - 419 °F
Zone 1 180 - 210 °C
356 - 410 °F
Zone 2 185 - 215 °C
365 - 419 °F
Zone 3 190 - 220 °C
374 - 428 °F
Zone 4 185 - 215 °C
365 - 419 °F
Dry Time 3.00 hour

@Temperature 100 °C
3.00 hour

@Temperature 212 °F