Polymer Property : Front Barrel Temperature = 285 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Front Barrel Temperature 250 - 285 °C
482 - 545 °F
Start Point: 270°C
Kingfa JH720 G10 10% Glass Fiber Reinforced PC
Features:High mechanical strengthGood size stabilityGood surfaceSuitable for exact moldingApplications:Exact mechanism partsPrinter, photocopies, scanner cabinetComputer plug partsCD-ROM, DVDElectri..
Front Barrel Temperature 270 - 285 °C
518 - 545 °F
Injection Molding
LG Chemical LUMID GN-2251BF Flame Retardant PA Alloy
Feature: Injection Molding, Flame Retardant PA AlloyApplication: E&E partsInformation provided by LG Chemical
Front Barrel Temperature 270 - 285 °C
518 - 545 °F
Injection Molding
LG Chemical LUMID GP2101BF PA66+GF10%, Halogen Free Flame Retardant
Feature: Injection Molding, PA66+GF10%, Halogen Free Flame RetardantApplication: ConnectorsCAS No. 32131-17-2, 25038-54-4, 65997-17-3, 88497-56-7, 1309-64-4 and 138265-88-0Information provided by LG..
Front Barrel Temperature 270 - 285 °C
518 - 545 °F
Injection Molding
LG Chemical LUMID GP2130B(W) PA66+GF13%, General Purpose
Feature: Injection Molding, PA66+GF13%, General PurposeApplication: Valve CoversCAS No. 32131-17-2, 65997-17-3 and 9010-79-9Information provided by LG Chemical
Front Barrel Temperature 270 - 285 °C
518 - 545 °F
Injection Molding
LG Chemical LUMID GP2151BF PA66+GF15%, Flame Retardant
Feature: Injection Molding, PA66+GF15%, Halogen Free Flame RetardantApplication: ConnectorsCAS No. 32131-17-2, 25038-54-4, 65997-17-3, 88497-56-7, 1309-64-4 and 138265-88-0Information provided by LG..
Front Barrel Temperature 270 - 285 °C
518 - 545 °F
Injection Molding
LG Chemical LUMID GP2200B(W) PA66+GF20%, General Purpose
Feature: Injection Molding, PA66+GF20%, General PurposeApplication: Automotive PartsCAS No. 32131-17-2 and 65997-17-3Information provided by LG Chemical
Front Barrel Temperature 270 - 285 °C
518 - 545 °F
Injection Molding
LG Chemical LUMID GP2251BF PA66+GF25%, Flame Retardant
Feature: Injection Molding, PA66+GF25%, Flame RetardantApplication: IT/OA (Micro Switch)CAS No. 32131-17-2, 65997-17-3, 88497-56-7, 1309-64-4 and 138265-88-0Information provided by LG Chemical
Front Barrel Temperature 270 - 285 °C
518 - 545 °F
Injection Molding
LG Chemical LUMID GP2301BF PA 66+GF30%, Flame Retardant
Feature: Injection Molding, PA 66+GF30%, Flame RetardantApplication: IT/OA (Micro Switch, ConnectorCAS No. 32131-17-2, 65997-17-3, 88497-56-7, 1309-64-4 and 138265-88-0Information provided by LG Che..
Front Barrel Temperature 270 - 285 °C
518 - 545 °F
Injection Molding
LG Chemical LUMID GP3200B(W) PA66+MF20%, General Purpose
Feature: Injection Molding, PA6+MF20%, General PurposeApplication: E&E (Rice Cooker Housing)Information provided by LG Chemical
Front Barrel Temperature 270 - 285 °C
518 - 545 °F
Injection Molding
LG Chemical LUMID GP3300B(W) PA66+MF30%, General Purpose
Feature: Injection Molding, PA66+MF30%, General PurposeApplication: Automotive (Engine Cover))CAS No. 25038-54-4 and 9010-79-1Information provided by LG Chemical
Front Barrel Temperature 270 - 285 °C
518 - 545 °F
Injection Molding
LG Chemical LUMID GP3400B(W) PA66+MF40%, General Purpose
Feature: Injection Molding, PA66+MF40%, General PurposeApplication: Automotive (Engine Cover)CAS No. 25038-54-4 and 14807-96-6Information provided by LG Chemical
Front Barrel Temperature 260 - 285 °C
500 - 545 °F
Injection Molding
LG Chemical LUMID HI2152A(W) PA6+GF15%, High Impact
Feature: Injection Molding, PA6+GF15%, High ImpactApplication: Automotive PartsCAS No. 25038-54-4, 9010-79-1 and 65997-17-3Information provided by LG Chemical
Front Barrel Temperature 270 - 285 °C
518 - 545 °F
Injection Molding
LG Chemical LUMID HI2202B(W) PA66+GF20%, High Impact
Feature: Injection Molding, PA66+GF20%, High ImpactApplication: Automotive (Covers)CAS No. 25038-54-4, 9010-79-1 and 65997-17-3Information provided by LG Chemical
Front Barrel Temperature 255 - 285 °C
491 - 545 °F
Injection Molding
LG Chemical LUMID LW4403A(W) PA66+GF/MF40%, Low Warpage
Feature: Injection Molding, PA66+GF/MF40%, Low WarpageApplication: Automotive (Timing Belt Cover)CAS No. 25038-54-4, 13983-17-0 and 65997-17-3Information provided by LG Chemical
Front Barrel Temperature 270 - 285 °C
518 - 545 °F
Injection Molding
LG Chemical LUPOY GN1006FT PC, Halogen Free, Flame Retardant
Description: Injection Molding, PC, Halogen Free Flame Retardant, Good FlowApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2Information provided by LG Chemical
Front Barrel Temperature 280 - 285 °C
536 - 545 °F
Solvay TECHNYL® A 60 G1 V30 PA66, 30% glass fiber, DRY
Description: Flame retardant Polyamide PA66 reinforced with 30% of glass fiber, for injection molding.Available in: Asia Pacific, Europe, Latin America and North AmericaProduct Applications: This R..
Front Barrel Temperature 279 - 285 °C
535 - 545 °F
Solvay Technyl® A20V25 25% Glass Filled, V-0 Nylon 66
Information provided by Rhodia; Rhodia has been acquired by Solvay.
Front Barrel Temperature 268 - 285 °C
515 - 545 °F
Teknor Apex Chemlon® 125-15 MGH Nylon 66, 25% Mineral Reinforced, 15% Glass Fiber Reinforced
Notes: 25% Mineral - 15% Glass; Excellent stiffness and strength, especially at high temperatures, with improved warpage control over glass reinforced products; FMVSS Flammability: Passes, FMVSS 302..
Front Barrel Temperature 263 - 285 °C
505 - 545 °F
Teknor Apex Chemlon® 133 GVH Nylon 66, 30% Glass Fiber Reinforced
Notes: Excellent for connectors and electrical parts; Flammability: Passes, FMVSS 302 Processing Method: Injection Molding Forms: PelletsInformation Provided by Teknor Apex
Front Barrel Temperature 275 - 285 °C
527 - 545 °F
Solvay TECHNYL® 2417IG PA66, 20% glass fiber, DRY
Description: Polyamide 66, 20% glass fiber reinforced, Impact modified for injection molding.Available in: Asia PacificProduct Applications: TECHNYL® 2417IG4 is used in all sectors of industries,..
Front Barrel Temperature 270 - 285 °C
518 - 545 °F
Zone 3
Eurostar Staramide RFB24 PA66, 20/10% Glass Fiber/Glass Bead Filled Injection Molded
RFB24 is a Glass Bead and Glass Fiber Reinforced, Polyamide 66 Injection Molding Resin (also known as Staramide 66 2010VK Z3)Information provided by Polymer Technology & Services, the North American..
Front Barrel Temperature 275 - 285 °C
527 - 545 °F
Zone 3
Eurostar Starflam AFR450X1 PA66, 25% Glass Filled, Injection Molded
AFR450X1 is a Red Phosphorous, Flame Retardant, Glass Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppli..
Front Barrel Temperature 275 - 285 °C
527 - 545 °F
Zone 3
Eurostar Starflam AFR450X2 PA66, 25% Glass Filled, Injection Molded
AFR450X2 is a Red Phosphorous, Flame Retardant, 25% Glass Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive su..
Front Barrel Temperature 275 - 285 °C
527 - 545 °F
Zone 3
Eurostar Starflam AFR470X2 PA66, 35% Glass Filled, Injection Molded
AFR470X2 is a Red Phosphorous, Flame Retardant, Glass Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppli..
Front Barrel Temperature 275 - 285 °C
527 - 545 °F
Solvay TECHNYL® 2210HS PA66, DRY
Description: Polyamide 66, unfilled, long-term stabilized, lubricated for injection molding.Available in: Asia Pacific Product Applications: TECHNYL® 2210HS is used in all sectors of industry, offe..
Front Barrel Temperature 255 - 285 °C
491 - 545 °F
Injection Molding
LG Chemical LUMID LW4009A(W) PA6+GF/MF40%, Low Warpage
Feature: Injection Molding, PA6+GF/MF40%, Low WarpageApplication: Automotive (Timing Belt Cover)CAS No. 25038-54-4, 13983-17-0 and 65997-17-3Information provided by LG Chemical