NYCOA 2237 Copolymer Nylon 6/66 Alloy

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Unreinforced
Manufacturer NYCOA, Inc.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NYCOA 2237 Copolymer Nylon 6/66 Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
transparent molding and extrusion gradeInformation provided by NYCOA, Inc.
Physical Properties Metric English Comments
Density 1.12 g/cc
0.0405 lb/in³
ISO 1183-A
Water Absorption 1.6 %
1.6 %
ISO METHOD 62
Linear Mold Shrinkage 0.015 cm/cm
0.015 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Yield 75.0 MPa
10900 psi
ISO METHOD 527
Elongation at Break >= 250 %
>= 250 %
ISO METHOD 527
Flexural Yield Strength 89.0 MPa
12900 psi
ISO METHOD 176
Flexural Modulus 2.261 GPa
327.9 ksi
ISO METHOD 178
Izod Impact, Notched 0.700 J/cm
1.31 ft-lb/in
ISO METHOD 180
Thermal Properties Metric English Comments
Melting Point 197 °C
387 °F
ISO METHOD 3146C
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified
Processing Properties Metric English Comments
Processing Temperature 250 °C
482 °F
Rear Barrel Temperature 200 °C
392 °F
Middle Barrel Temperature 230 °C
446 °F
Front Barrel Temperature 250 °C
482 °F
Nozzle Temperature 250 °C
482 °F
Mold Temperature 80.0 °C
176 °F
Drying Temperature 76.0 °C
169 °F