NYCOA 1637 PA 6

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Heat Stabilized
Manufacturer NYCOA, Inc.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NYCOA 1637 PA 6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
plasticized and heat stabilized extrusion grade for the wire jacketing industry to 7,000+ fpm. UL Flammability Component listing for use as cable jacketing.Information provided by NYCOA, Inc.
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
ASTM D792
Water Absorption 2.5 %
2.5 %
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell R 105
105
ASTM D785
Tensile Strength, Yield 73.0 MPa
10600 psi
ASTM D638
Elongation at Break 150 %
150 %
ASTM D638
Flexural Yield Strength 76.0 MPa
11000 psi
ASTM D790
Flexural Modulus 2.10 GPa
305 ksi
ASTM D790
Izod Impact, Notched 0.530 J/cm
0.993 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 215 °C
419 °F
ASTM D789
Deflection Temperature at 1.8 MPa (264 psi) 54.0 °C
129 °F
ASTM D648
Processing Properties Metric English Comments
Processing Temperature 250 °C
482 °F
Rear Barrel Temperature 215 °C
419 °F
Middle Barrel Temperature 230 °C
446 °F
Front Barrel Temperature 250 °C
482 °F
Drying Temperature 76.0 °C
169 °F