Material Notes:
Versaflex™ HC MT555 is an easy processing material designed for applications where FDA compliance and medical testing is required. - Excellent Colorability - Soft TouchRear: 340 - 360F Center: 380 - 400F Front: 390 - 410F Screw: 80 - 200 RPMsColor concentrates with polypropylene, ethylene vinyl acetate, or low density polyethylene carriers are most suitable for coloring Versaflex™ HC MT555. Improved color dispersion can be achieved by using higher melt flow concentrates (with a melt flow from 25 - 40 g/10 min). Typical loadings for color concentrates are 1% to 5% by weight. Liquid color can be used, but mineral oil based carriers may have an effect on the final hardness value. Concentrates based on PVC should not be used. A high color match consistency can be obtained by using precolored compounds available from GLS. The final determination of color concentrate suitability should be determined by customer trials. Purge thoroughly before and after use of this product with a low flow (0.5 - 2.5 MFR) polyethylene or polypropylene. Regrind levels up to 20% can be used with Versaflex™ HC MT555 with minimal property loss, provided that the regrind is free of contamination. To minimize losses during molding, the melt temperature should remain as low as possible. The final determination of regrind effectiveness should be determined by the customer. Versaflex™ HC MT555 has excellent melt stability. Maximum residence times may vary, depending on the size of the barrel. Generally, the barrel should be emptied if it is idle for periods of 8 - 10 minutes or longer. Drying is not Required Injection Speed: 1 to 5 in/sec 1st Stage - Boost Pressure: 100 to 800 psi 2nd Stage - Hold Pressure: 20% of Boost Hold Time (Thick Part): 4 to 10 sec Hold Time (Thin Part): 1 to 4 secInformation provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 0.888 g/cc
0.888 g/cc
ASTM D792
Viscosity 13100 cP

@Shear Rate 11200 1/s,
Temperature 200 °C
13100 cP

@Shear Rate 11200 1/s,
Temperature 392 °F
ASTM D3835
73000 cP

@Shear Rate 1340 1/s,
Temperature 200 °C
73000 cP

@Shear Rate 1340 1/s,
Temperature 392 °F
ASTM D3835
Linear Mold Shrinkage, Flow 0.016 - 0.022 cm/cm
0.016 - 0.022 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore A 54
54
10 sec; ASTM D2240
Tensile Strength at Break 6.38 MPa

@Temperature 23.0 °C
925 psi

@Temperature 73.4 °F
Die C2 hr; ASTM D412
Tensile Stress 1.74 MPa

@Strain 100 %,
Temperature 23.0 °C
252 psi

@Strain 100 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
3.31 MPa

@Strain 300 %,
Temperature 23.0 °C
480 psi

@Strain 300 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
Elongation at Break 630 %

@Temperature 23.0 °C
630 %

@Temperature 73.4 °F
Die C2 hr; ASTM D412
Compression Set 20 %

@Temperature 23.0 °C,
Time 79200 sec
20 %

@Temperature 73.4 °F,
Time 22.0 hour
ASTM D395B
Processing Properties Metric English Comments
Rear Barrel Temperature 166 - 182 °C
331 - 360 °F
Middle Barrel Temperature 182 - 204 °C
360 - 399 °F
Front Barrel Temperature 188 - 210 °C
370 - 410 °F
Nozzle Temperature 188 - 210 °C
370 - 410 °F
Die Temperature 193 - 204 °C
379 - 399 °F
Melt Temperature 193 - 204 °C
379 - 399 °F
193 - 221 °C
379 - 430 °F
Mold Temperature 15.6 - 26.7 °C
60.1 - 80.1 °F
Back Pressure 0.000 - 0.552 MPa
0.000 - 80.1 psi
Screw Speed 80 - 120 rpm
80 - 120 rpm
Descriptive Properties Value Comments
Agency Ratings FDA 21 CFR 177.1210
Please contact GLS Thermoplastic Elastomers for the specific FDA compliance letter on this product.
ISO 10993 Part 4
ISO 10993 Part 5
USP Class VI
Appearance Translucent
Features Good Colorability
Good Processability
Good Processing Stability
Forms Pellets
Generic Material TPE
Generic Name Thermoplastic Elastomer (TPE)
Manufacturer / Supplier GLS Thermoplastic Elastomers
Processing Method Extrusion
Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
RoHS Compliance RoHS Compliant
Suggested Max Regrind 20%
Uses Medical/Healthcare Applications
Personal Care
Transparent or Translucent Parts
Tubing