Teknor Apex Flexalloy® 9100-75 Polyvinyl Chloride Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Vinyl (PVC)
Manufacturer Teknor Apex Company
Trade Name Flexalloy®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex Flexalloy® 9100-75 Polyvinyl Chloride Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Good Flexibility, General Purpose, Ultra High MW, Recyclable, Good Thermal Stability, Good Weather ResistanceUses- Footwear, Tubing, Gaskets, Weatherstripping, hose, Wheels, SealsForms-PelletsProcessing-Extrusion, Injection MoldingInformation provided by Teknor Apex Company
Physical Properties Metric English Comments
Specific Gravity 1.18 g/cc
1.18 g/cc
23°C; ASTM D792
Linear Mold Shrinkage 0.010 - 0.025 cm/cm
0.010 - 0.025 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore A 75
75
15 seconds; ASTM D2240
Tensile Strength, Yield 8.27 MPa
1200 psi
100%; ASTM D412
17.2 MPa
2500 psi
ASTM D412
Elongation at Break 350 %
350 %
ASTM D412
Tear Strength 36.8 kN/m
210 pli
Die C; ASTM D624
Compression Set 26 %
26 %
73°F, 22 hr.; ASTM D395
55 %
55 %
158°F, 22 hr.; ASTM D395
Thermal Properties Metric English Comments
Brittleness Temperature -48.0 °C
-54.4 °F
ASTM D746
Processing Properties Metric English Comments
Rear Barrel Temperature 182 - 199 °C
360 - 390 °F
Middle Barrel Temperature 182 - 199 °C
360 - 390 °F
Front Barrel Temperature 182 - 199 °C
360 - 390 °F
Mold Temperature 23.9 - 51.7 °C
75.0 - 125 °F
Back Pressure 0.345 - 1.03 MPa
50.0 - 150 psi
Descriptive Properties Value Comments
Screw Compression Ratio 2:1-3:1
Screw L/D Ratio 20:1- 24:1
Suggested Max Regrind, % 20