Polymer Property : Zone 1 = 338 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Zone 1 155 - 170 °C
311 - 338 °F
Extrusion Molding
Kolon ELLAS K-429A Ester Based Thermoplastic Polyurethane
ApplicationsIndustry PartsOutsole of Soccer ShoeHighly Pressurized Hose Information provided by API-Kolon.
Zone 1 155 - 170 °C
311 - 338 °F
Extrusion Molding
Kolon ELLAS K-480A Ester Based Thermoplastic Polyurethane
ApplicationsExtrusionInjectionCompoundingIndustry PartsParts for Automobile/Mobile phoneAcetal Compound Information provided by API-Kolon.
Zone 1 155 - 170 °C
311 - 338 °F
Injection Molding
Kolon ELLAS K-490AB Ester Based Thermoplastic Polyurethane
ApplicationsExtrusionInjectionFilm/SeatBlown filmIndustry Parts Information provided by API-Kolon.
Zone 1 155 - 170 °C
311 - 338 °F
Extrusion Molding
Kolon ELLAS K-490AB Ester Based Thermoplastic Polyurethane
ApplicationsExtrusionInjectionFilm/SeatBlown filmIndustry Parts Information provided by API-Kolon.
Zone 1 150 - 170 °C
302 - 338 °F
Injection Molding
Kolon ELLAS K-785A Ester Based Thermoplastic Polyurethane
ApplicationsCompoundingFilm/SeatT-DIE High Frequency FilmPVC/Rubber Compound Information provided by API-Kolon.
Zone 1 150 - 170 °C
302 - 338 °F
Injection Molding
Kolon ELLAS K-787A Ester Based Thermoplastic Polyurethane
ApplicationsExtrusionInjectionFlexible HoseIndustry Parts Information provided by API-Kolon.
Zone 1 160 - 170 °C
320 - 338 °F
Silon Taborex TA 1109 MD Chemically-Crosslinkable MDPE Compound
TABOREX TA 1110 MD is a crosslinkable compound made by a Silane grafted ethylene polymer. This graft polymer constitutes together with a Masterbatch containing the crosslinking catalyst a “SIOP..
Zone 1 160 - 170 °C
320 - 338 °F
Silon Taborex TA 1117HD Chemically-Crosslinkable HDPE Compound
TABOREX TA 1117 HD is a crosslinkable compound made by Silane grafted ethylene polymer. This graft polymer constitutes together with a Masterbatch containing the crosslinking catalyst a “SIOPLA..
Zone 1 160 - 170 °C
320 - 338 °F
Silon Taborex TA 1131 HD Chemically-Crosslinkable HDPE Compound
TABOREX TA 1131 HD is a crosslinkable compound made by Silane grafted ethylene polymer. This graft polymer constitutes together with a Masterbatch containing the crosslinking catalyst a “SIOPLA..
Zone 1 160 - 170 °C
320 - 338 °F
Silon Taborex TA 1132 HD Chemically-Crosslinkable HDPE Compound
TABOREX TA 1132 HD is a crosslinkable compound made of Silane grafted ethylene polymer. This graft polymer constitutes together with a Masterbatch containing the crosslinking catalyst a “SIOPLA..
Zone 1 160 - 170 °C
320 - 338 °F
Silon Taborex TA 1133 HD Chemically-Crosslinkable HDPE Compound
TABOREX TA 1133 HD is a crosslinkable compound made of Silane grafted ethylene polymer. This graft polymer constitutes together with a Masterbatch containing the crosslinking catalyst a “SIOPLA..
Zone 1 160 - 170 °C
320 - 338 °F
Silon Taborex TA 1134 HD Chemically-Crosslinkable HDPE Compound
TABOREX TA 1134 HD is a crosslinkable compound made of Silane grafted ethylene polymer. This graft polymer constitutes together with a Masterbatch containing the crosslinking catalyst a “SIOPLA..
Zone 1 160 - 170 °C
320 - 338 °F
Silon Taborex TA 1135 HD Chemically-Crosslinkable HDPE Compound
TABOREX TA 1135 HD is a crosslinkable compound made by Silane grafted ethylene polymer. This graft polymer constitutes together with a Masterbatch containing the crosslinking catalyst a “SIOPLA..
Zone 1 160 - 170 °C
320 - 338 °F
Silon Taborex TA 1108 HD Chemically-Crosslinkable HDPE Compound
TABOREX TA 1108 HD is a crosslinkable compound according to the “SIOPLAS-SYSTEM”; made by a Silane grafted ethylene copolymer known as the graft and a Masterbatch containing the crosslinki..
Zone 1 160 - 170 °C
320 - 338 °F
Eurostar Starflam MX06101 PP, Flame Retardant, Injection Molding
Starflam MX06101 is an Unfilled, Halogen Free Flame Retardant Polypropylene Injection Molding ResinInformation provided by Eurostar.