Processing Properties Metric English Comments
Pot Life 40.0 - 50.0 min

@Temperature 50.0 - 50.0 °C
40.0 - 50.0 min

@Temperature 122 - 122 °F
Average value: 45.0 min Grade Count:1
Overview of materials for Thermoset Polyurethane, Adhesive
This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Adhesive". Each property range of values reported is minimum and maximum values ..
Pot Life 40.0 - 60.0 min

@Temperature 23.0 °C
40.0 - 60.0 min

@Temperature 73.4 °F
TSE Industries EcoWIND® P200G High Performance Filament Winding Polyurethane Resin for Pipes
TSE-EcoWIND® resins are “Environmentally-Preferred Products” or EPP’s. They are a pair of polyurethane resins free of Styrene, and are “ultra-low” emitting during application. TSE-EcoWIND® re..
Pot Life 40.0 min

@Temperature 25.0 °C
40.0 min

@Temperature 77.0 °F
100 grams
Cytec (Conap) FR-2000 / FR-200 Conapoxy® Resin / Conacure® Hardener
Epoxy Potting and Encapsulating Systems for Electronic ApplicationsHigh technology epoxy resin systems for potting and encapsulation, for the defense, aerospace, electronics, computer, automotive an..
Pot Life 40.0 min

@Temperature 25.0 °C
40.0 min

@Temperature 77.0 °F
100 grams
Cytec (Conap) RN-1200 / EA-028 Conapoxy® Resin / Conacure® Hardener
Epoxy Potting and Encapsulating Systems for Electronic ApplicationsHigh technology epoxy resin systems for potting and encapsulation, for the defense, aerospace, electronics, computer, automotive an..
Pot Life 40.0 min

@Temperature 25.0 °C
40.0 min

@Temperature 77.0 °F
100 grams
Cytec (Conap) RN-1210 / EA-028 Conapoxy® Resin / Conacure® Hardener
Epoxy Potting and Encapsulating Systems for Electronic ApplicationsHigh technology epoxy resin systems for potting and encapsulation, for the defense, aerospace, electronics, computer, automotive an..
Pot Life 40.0 min

@Temperature 25.0 °C
40.0 min

@Temperature 77.0 °F
0.5 lbm
Cytec EN-12 (Conap) Casting, Potting, and Molding Compound
High Technology Potting, Casting and Molding CompoundsTwo-component, polybutadiene-based liquid urethane casting and potting systems. When reacted these high technology systems produce tough, stable..
Pot Life 40.0 min

@Temperature 23.9 °C
40.0 min

@Temperature 75.0 °F
Devcon Brushable Ceramic - Red, Blue Epoxy
Precision Repair EpoxyComments: Low-viscosity, alumina-filled, brushable epoxy compound, when applied to a 15-20 mil coating, provides a smooth, protective barrier against wear, abrasion, corrosion,..
Pot Life 40.0 min

@Temperature 23.9 °C
40.0 min

@Temperature 75.0 °F
Devcon Sprayable Ceramic™ Epoxy
Precision Repair EpoxyComments: A sprayable ceramic-reinforced composite that can be sprayed in a manner similar to high-solid paints. Ideal for protecting pumps, paper machines, stacks, pump pads,..
Pot Life 40.0 - 50.0 min

@Temperature 50.0 °C
40.0 - 50.0 min

@Temperature 122 °F
1 lbm
Cytec EN-2555 (Conap) Potting and Encapsulation Adhesive
Polyurethane Potting and Encapsulating SystemsConathane® EN-2500 series polyurethane potting and encapsulating systems from Cytek have varying degrees of worklife, viscosity and hardness for many s..
Pot Life <= 40.0 min

@Temperature 25.0 °C
<= 40.0 min

@Temperature 77.0 °F
100 g
Armstrong A-31 Epoxy Adhesive
Is a neutral-colored thixotropic paste material having a creamy or buttery consistency that will not flow even when cured at elevated temperatures A-31 also features Extremely low outgassing charact..
Pot Life <= 40.0 min

@Temperature 25.0 °C
<= 40.0 min

@Temperature 77.0 °F
100 g
Armstrong C-1/H20 Epoxy Adhesive
A versatile, low viscosity, unfilled resin used for electrical potting and laminating applications. It is an excellent insulator, and provides outstanding chemical resistance to most compoundsInfor..
Pot Life <= 40.0 min

@Temperature 25.0 °C
<= 40.0 min

@Temperature 77.0 °F
100 g
Armstrong C-4/D Epoxy Adhesive
A low viscosity, clear amber, unfilled adhesive, recommended for use with activators D or W. C-4 with Activator W offers maximum versatility in that differing degrees of flexibility can be achieved ..
Pot Life 40.0 min

@Temperature 75.0 °C
40.0 min

@Temperature 167 °F
ACC EP RAP 45 EPI Engineered Polymers Aliphatic Polyurea
EP RAP 45 Aliphatic Polyurea, “Powered by Reactamine® Technology”, is a two component 100% solids, no VOC is, aliphatic polyurea (silicone optional) coating, that was developed for UV stable (col..
Pot Life 40.0 min

@Temperature 75.0 °C
40.0 min

@Temperature 167 °F
ACC EP RAP-1567 EPI Engineered Polymers Aliphatic Polyurea
RAP-1567 HX is a two component 100% solids, no VOC’s, aliphatic polyureas “Powered by ReactAmine® Technology” that was developed for UV stable (colorfast) polyurea applications. This new generat..
Pot Life 40.0 min

@Temperature 75.0 °C
40.0 min

@Temperature 167 °F
ACC EP RAP-1567 HX EPI Engineered Polymers Aliphatic Polyurea
RAP-1567 is a two component 100% solids, no VOC’s, aliphatic polyureas “Powered by ReactAmine® Technology” that was developed for UV stable (colorfast) polyurea applications. This new generation..
Pot Life 40.0 min

@Temperature 75.0 °C
40.0 min

@Temperature 167 °F
ACC EP RAP-1567 SP-HX EPI Engineered Polymers Silicone Aliphatic Polyurea
RAP-1567 SP is a two component 100% solids, no VOC’s, silicone aliphatic polyureas “Powered by ReactAmine® Technology” that was developed for UV stable (colorfast) polyurea applications. This ne..
Pot Life 40.0 min

@Temperature 75.0 °C
40.0 min

@Temperature 167 °F
ACC EP RAP-1567 SP-HX EPI Engineered Polymers Silicone Aliphatic Polyurea
RAP-1567 SP-HX is a two component 100% solids, no VOC’s, silicone aliphatic polyureas “Powered by ReactAmine® Technology” that was developed for UV stable (colorfast) polyurea applications. This..
Pot Life 40.0 min

@Temperature 75.0 °C
40.0 min

@Temperature 167 °F
ACC EP RAP 45 14 EPI Engineered Polymers Aliphatic Polyurea
EP RAP 45 14 Aliphatic Polyurea, “Powered by Reactamine® Technology”, is a two component 100% solids, no VOC’s, aliphatic polyurea coating that was developed for UV stable (colorfast) polyurea f..
Pot Life 40.0 - 60.0 min

@Temperature 23.0 °C
40.0 - 60.0 min

@Temperature 73.4 °F
TSE Industries EcoWIND® P200G High Performance Filament Winding Polyurethane Resin for Pipes