Devcon Brushable Ceramic - Red, Blue Epoxy

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Adhesive
Manufacturer Devcon
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Devcon Brushable Ceramic - Red, Blue Epoxy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Precision Repair EpoxyComments: Low-viscosity, alumina-filled, brushable epoxy compound, when applied to a 15-20 mil coating, provides a smooth, protective barrier against wear, abrasion, corrosion, erosion and chemical attack. Temperature range up to 350°F. White is NSF-certified for use in potable water applications. Low friction surface reduces turbulence, wear and cavitations. Red and white formulas are USDA-approved. Outstanding chemical resistance to acids, solvents and alkalis.Data provided by Ellsworth Adhesives.
Physical Properties Metric English Comments
Density 1.68 g/cc
0.0606 lb/in³
Viscosity 32000 cP
32000 cP
with hardener
Mechanical Properties Metric English Comments
Hardness, Shore D 90
90
ASTM D2240
Tensile Strength, Ultimate 26.2 MPa
3800 psi
ASTM D638
Modulus of Elasticity 6.21 GPa
900 ksi
In Tension; ASTM D638
Flexural Yield Strength 55.2 MPa
8000 psi
ASTM D790
Compressive Yield Strength 105 MPa
15200 psi
ASTM D695
Adhesive Bond Strength 13.8 MPa
2000 psi
Adhesive tensile shear strength; ASTM D1002
Thermal Properties Metric English Comments
CTE, linear 34.0 µm/m-°C

@Temperature 20.0 °C
18.9 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Thermal Conductivity 0.803 W/m-K
5.57 BTU-in/hr-ft²-°F
ASTM C177
Maximum Service Temperature, Air 177 °C
350 °F
Operating Temperature
Shrinkage 0.20 %
0.20 %
During Cure; ASTM D2566
Electrical Properties Metric English Comments
Dielectric Constant 38.7
38.7
ASTM D150
Dielectric Strength 15.0 kV/mm
382 kV/in
ASTM D149
Processing Properties Metric English Comments
Processing Temperature 21.1 °C
70.0 °F
Pot Life 40.0 min

@Temperature 23.9 °C
40.0 min

@Temperature 75.0 °F
Descriptive Properties Value Comments
Coverage per lb. 66 in²
at 1/4 inch thick
Mix Ratio by Volume 3.4 to 1
resin:hardener
Mix Ratio By Weight 5.6 to 1
resin:hardener