Category Polymer , Thermoset , Polyurethane, TS , Thermoset Polyurethane, Liquid
Manufacturer TSE Industries, Inc
Trade Name EcoWIND®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TSE Industries EcoWIND® P200G High Performance Filament Winding Polyurethane Resin for Pipes.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TSE-EcoWIND® resins are “Environmentally-Preferred Products” or EPP’s. They are a pair of polyurethane resins free of Styrene, and are “ultra-low” emitting during application. TSE-EcoWIND® resins are formulated for filament winding applications serving the composite pressure vessel, tank, and piping markets. These PU resins have tested positively in both hot and cold pressure vessel applications and can be applied to reinforce thermoplastic substrates (i.e. polyethylene, ABS, etc.) or applied directly to a release coated mandrel surface.All information provided by TSE Industries
Physical Properties Metric English Comments
Viscosity 100 - 300 cP

@Temperature 75.0 °C
100 - 300 cP

@Temperature 167 °F
Mechanical Properties Metric English Comments
Tensile Strength, Yield 89.0 MPa
12900 psi
Plain Cast Resin; ASTM D638
Elongation at Break 5.0 - 6.0 %
5.0 - 6.0 %
Plain Cast Resin; ASTM D638
Modulus of Elasticity 3.00 GPa
435 ksi
Plain Cast Resin; ASTM D638
Flexural Yield Strength 115 MPa
16700 psi
Plain Cast Resin; ASTM D790
Flexural Modulus 2.80 GPa
406 ksi
Plain Cast Resin; ASTM D790
Izod Impact, Notched 4.78 J/cm
8.95 ft-lb/in
Plain Cast Resin; ASTM D256
Charpy Impact, Notched 0.230 J/cm²
1.09 ft-lb/in²
Plain Cast Resin
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 136 °C
277 °F
Plain Cast Resin; ASTM D648
Glass Transition Temp, Tg 145 °C
293 °F
Plain Cast Resin; ASTM D3418
Processing Properties Metric English Comments
Pot Life 40.0 - 60.0 min

@Temperature 23.0 °C
40.0 - 60.0 min

@Temperature 73.4 °F