Processing Properties | Metric | English | Comments |
---|---|---|---|
Pot Life | 40.0 - 50.0 min @Temperature 50.0 - 50.0 °C |
40.0 - 50.0 min @Temperature 122 - 122 °F |
Average value: 45.0 min Grade Count:1 |
Overview of materials for Thermoset Polyurethane, Adhesive This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Adhesive". Each property range of values reported is minimum and maximum values .. |
|||
Pot Life | 40.0 - 60.0 min @Temperature 23.0 °C |
40.0 - 60.0 min @Temperature 73.4 °F |
|
TSE Industries EcoWIND® P200G High Performance Filament Winding Polyurethane Resin for Pipes TSE-EcoWIND® resins are “Environmentally-Preferred Products” or EPP’s. They are a pair of polyurethane resins free of Styrene, and are “ultra-low” emitting during application. TSE-EcoWIND® re.. |
|||
Pot Life | 40.0 min @Temperature 25.0 °C |
40.0 min @Temperature 77.0 °F |
100 grams |
Cytec (Conap) FR-2000 / FR-200 Conapoxy® Resin / Conacure® Hardener Epoxy Potting and Encapsulating Systems for Electronic ApplicationsHigh technology epoxy resin systems for potting and encapsulation, for the defense, aerospace, electronics, computer, automotive an.. |
|||
Pot Life | 40.0 min @Temperature 25.0 °C |
40.0 min @Temperature 77.0 °F |
100 grams |
Cytec (Conap) RN-1200 / EA-028 Conapoxy® Resin / Conacure® Hardener Epoxy Potting and Encapsulating Systems for Electronic ApplicationsHigh technology epoxy resin systems for potting and encapsulation, for the defense, aerospace, electronics, computer, automotive an.. |
|||
Pot Life | 40.0 min @Temperature 25.0 °C |
40.0 min @Temperature 77.0 °F |
100 grams |
Cytec (Conap) RN-1210 / EA-028 Conapoxy® Resin / Conacure® Hardener Epoxy Potting and Encapsulating Systems for Electronic ApplicationsHigh technology epoxy resin systems for potting and encapsulation, for the defense, aerospace, electronics, computer, automotive an.. |
|||
Pot Life | 40.0 min @Temperature 25.0 °C |
40.0 min @Temperature 77.0 °F |
0.5 lbm |
Cytec EN-12 (Conap) Casting, Potting, and Molding Compound High Technology Potting, Casting and Molding CompoundsTwo-component, polybutadiene-based liquid urethane casting and potting systems. When reacted these high technology systems produce tough, stable.. |
|||
Pot Life | 40.0 min @Temperature 23.9 °C |
40.0 min @Temperature 75.0 °F |
|
Devcon Brushable Ceramic - Red, Blue Epoxy Precision Repair EpoxyComments: Low-viscosity, alumina-filled, brushable epoxy compound, when applied to a 15-20 mil coating, provides a smooth, protective barrier against wear, abrasion, corrosion,.. |
|||
Pot Life | 40.0 min @Temperature 23.9 °C |
40.0 min @Temperature 75.0 °F |
|
Devcon Sprayable Ceramic™ Epoxy Precision Repair EpoxyComments: A sprayable ceramic-reinforced composite that can be sprayed in a manner similar to high-solid paints. Ideal for protecting pumps, paper machines, stacks, pump pads,.. |
|||
Pot Life | 40.0 - 50.0 min @Temperature 50.0 °C |
40.0 - 50.0 min @Temperature 122 °F |
1 lbm |
Cytec EN-2555 (Conap) Potting and Encapsulation Adhesive Polyurethane Potting and Encapsulating SystemsConathane® EN-2500 series polyurethane potting and encapsulating systems from Cytek have varying degrees of worklife, viscosity and hardness for many s.. |
|||
Pot Life | <= 40.0 min @Temperature 25.0 °C |
<= 40.0 min @Temperature 77.0 °F |
100 g |
Armstrong A-31 Epoxy Adhesive Is a neutral-colored thixotropic paste material having a creamy or buttery consistency that will not flow even when cured at elevated temperatures A-31 also features Extremely low outgassing charact.. |
|||
Pot Life | <= 40.0 min @Temperature 25.0 °C |
<= 40.0 min @Temperature 77.0 °F |
100 g |
Armstrong C-1/H20 Epoxy Adhesive A versatile, low viscosity, unfilled resin used for electrical potting and laminating applications. It is an excellent insulator, and provides outstanding chemical resistance to most compoundsInfor.. |
|||
Pot Life | <= 40.0 min @Temperature 25.0 °C |
<= 40.0 min @Temperature 77.0 °F |
100 g |
Armstrong C-4/D Epoxy Adhesive A low viscosity, clear amber, unfilled adhesive, recommended for use with activators D or W. C-4 with Activator W offers maximum versatility in that differing degrees of flexibility can be achieved .. |
|||
Pot Life | 40.0 min @Temperature 75.0 °C |
40.0 min @Temperature 167 °F |
|
ACC EP RAP 45 EPI Engineered Polymers Aliphatic Polyurea EP RAP 45 Aliphatic Polyurea, “Powered by Reactamine® Technology”, is a two component 100% solids, no VOC is, aliphatic polyurea (silicone optional) coating, that was developed for UV stable (col.. |
|||
Pot Life | 40.0 min @Temperature 75.0 °C |
40.0 min @Temperature 167 °F |
|
ACC EP RAP-1567 EPI Engineered Polymers Aliphatic Polyurea RAP-1567 HX is a two component 100% solids, no VOC’s, aliphatic polyureas “Powered by ReactAmine® Technology” that was developed for UV stable (colorfast) polyurea applications. This new generat.. |
|||
Pot Life | 40.0 min @Temperature 75.0 °C |
40.0 min @Temperature 167 °F |
|
ACC EP RAP-1567 HX EPI Engineered Polymers Aliphatic Polyurea RAP-1567 is a two component 100% solids, no VOC’s, aliphatic polyureas “Powered by ReactAmine® Technology” that was developed for UV stable (colorfast) polyurea applications. This new generation.. |
|||
Pot Life | 40.0 min @Temperature 75.0 °C |
40.0 min @Temperature 167 °F |
|
ACC EP RAP-1567 SP-HX EPI Engineered Polymers Silicone Aliphatic Polyurea RAP-1567 SP is a two component 100% solids, no VOC’s, silicone aliphatic polyureas “Powered by ReactAmine® Technology” that was developed for UV stable (colorfast) polyurea applications. This ne.. |
|||
Pot Life | 40.0 min @Temperature 75.0 °C |
40.0 min @Temperature 167 °F |
|
ACC EP RAP-1567 SP-HX EPI Engineered Polymers Silicone Aliphatic Polyurea RAP-1567 SP-HX is a two component 100% solids, no VOC’s, silicone aliphatic polyureas “Powered by ReactAmine® Technology” that was developed for UV stable (colorfast) polyurea applications. This.. |
|||
Pot Life | 40.0 min @Temperature 75.0 °C |
40.0 min @Temperature 167 °F |
|
ACC EP RAP 45 14 EPI Engineered Polymers Aliphatic Polyurea EP RAP 45 14 Aliphatic Polyurea, “Powered by Reactamine® Technology”, is a two component 100% solids, no VOC’s, aliphatic polyurea coating that was developed for UV stable (colorfast) polyurea f.. |
|||
Pot Life | 40.0 - 60.0 min @Temperature 23.0 °C |
40.0 - 60.0 min @Temperature 73.4 °F |
|
TSE Industries EcoWIND® P200G High Performance Filament Winding Polyurethane Resin for Pipes TSE-EcoWIND® resins are “Environmentally-Preferred Products” or EPP’s. They are a pair of polyurethane resins free of Styrene, and are “ultra-low” emitting during application. TSE-EcoWIND® re.. |