Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Pot Life = 10 min Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Pot Life 10 - 15 min
10 - 15 min
Mass: 50g
Resinlab® EP1112 Clear Electronic Grade Epoxy Encapsulant
Resinlab™ EP 1112 Clear is a two part unfilled fast curing electronic grade epoxy encapsulant designed for small to medium sized castings. It cures completely at room temperature to a tough, flexib..
Pot Life 10 - 20 min
10 - 20 min
Mass: 50g; TM R050-19
Resinlab® EP1225 Black Unfilled Epoxy Adhesive
Resinlab™ EP1225 Black is a two part unfilled epoxy adhesive designed for bonding of metals, ceramics and most plastics. It has slightly thixotropic viscosity to give gap filling ability bust stil..
Pot Life 10 - 20 min
10 - 20 min
Time before parts must be mated
Lord Adhesives 320 Toughened, High Viscosity SMC, FRP, General Purpose Epoxy Adhesive
Lord Epoxy AdhesivesLord® Epoxy Adhesives create superior bonds for rubber, SMC, plastics and metals. Our epoxy adhesives are widely used in the automotive industry, over 10 million cars and ligh..
Pot Life 10 min
10 min
Taiwan PU Corporation PPG CPU-1090C Polyurethane Casting Elastomer
A urethane elastomer that can be cured by reacting with a polyamine or a polyolhardener. The molding process is composed of pre-heating, degassing, maxing with a hardener, pouring into the mold, cu..
Pot Life 10 min
10 min
Curing
Silikony Polskie Polastosil M-99 Silicone Rubber
Rubber with strong hardness
Pot Life 10 - 15 min
10 - 15 min
100 gram batch
Master Bond EP41S Fast Curing Epoxy Features Chemical Resistance
Description: Master Bond EP41S is a two component epoxy resin compound for durable, high performance, tough, high strength coatings, liners and sealants with outstanding resistance to organic solven..
Pot Life 10 - 15 min
10 - 15 min
100 gram mass
Master Bond EP41SMed Two Component, Low Viscosity, USP Class VI Epoxy System
Master Bond Polymer Adhesive EP41S Medical is a two component low viscosity epoxy resin system for high performance bonding, sealing, coating, as well as small encapsulations, pottings and castings...
Pot Life 10 min

@Temperature 25.0 °C
10 min

@Temperature 77.0 °F
Trelleborg Emerson & Cuming EP679 Patch Paste
Blue patch pasteAll information provided by Trelleborg Emerson & Cuming
Pot Life 10 min
10 min
Epoxy Technology EPO-TEK® 302 Fast Setting, Optical Epoxy
Product Description: EPO-TEK® 302 is a two component, fast-gelling, room temperature curing epoxy, designed for electronic, optical, medical, and general applications. Advantages & Application No..
Pot Life 10 min
10 min
Epoxyset Epoxiohm EO-30FST Electrically Conductive Epoxy Adhesive
EO-30-FST is two part, fast cure, silver filled, and high electrical conductivity epoxy adhesive. Both components are silver filled permitting a simple 1:1 mix ratio by weight. It has smooth creamy ..
Pot Life 10 - 12 min

@Temperature 24.0 °C
10 - 12 min

@Temperature 75.2 °F
12-14 minutes gel time, ASTM-D-2471, 1/2lb mass
BCC Products DP-11-88 Urethane Adhesive
DP-11-88 is a medium viscosity quick setting easy to use urethane adhesive. This system was specifically designed to bond together the MB2001/MB3000 Model/Tooling Board to create desired dimensions ..
Pot Life 10 min
10 min
Tra-Con Tra-Bond FS411 Fast Cure Epoxy Adhesive System
TRA-BOND FS-411 is an exceptional epoxy formulation recommended for lower temperature or wet industrial bonding applications where FAST CURING is required. It was designed to have low outgassing in ..
Pot Life 10 - 15 min
10 - 15 min
Mass: 50g
Resinlab® EP1112 Black Electronic Grade Epoxy Encapsulant
Resinlab™ EP 1112 Black is a two part unfilled fast curing electronic grade epoxy encapsulant designed for small to medium sized castings. It cures completely at room temperature to a tough, flexib..
Pot Life 10 min
10 min
Mass: 50g
Resinlab® UR3001 Clear Two Part Urethane Encapsulant
Resinlab™ UR 3001 is a clear, two component, room temperature curing urethane encapsulating system. It is designed to cure completely at room temperature. UR 3001 provides excellent environmental p..
Pot Life 10 - 20 min
10 - 20 min
Mass: 100g
Resinlab® UR3005 Clear Two Part Urethane Elastomer
Resinlab™ UR 3005 Clear is a two component, room temperature curing polybutadiene polyurethane casting and potting system. It is designed to cure completely at room temperature. UR 3005 Clear provi..
Pot Life 10 - 20 min
10 - 20 min
Mass: 100g
Resinlab® UR3005 Two Part Urethane Elastomer
Resinlab™ UR 3005 is a two component, room temperature curing polybutadiene polyurethane casting and potting system. It is designed to cure completely at room temperature. UR 3005 provides excellen..
Pot Life 10 min
10 min
Loctite® Durabond® U-10FL Urethane Adhesive
Urethane AdhesivesLoctite offers a complete line of one-part and two-part epoxy and urethane adhesives for structural bonding, potting and encapsulating. The Loctite® Durabond® line contains 14 ap..
Pot Life 10 - 15 min
10 - 15 min
Mass: 50g; TM R050-19
Resinlab® EP1305 Black Highly Toughened Urethane Modified Epoxy
Resinlab™ EP1305 Black is a highly toughened urethane modified epoxy designed for bonding PVC, metals, ceramics and other difficult to bond substrates. The system has a thixotropic non-sag viscosi..
Copyright © lookpolymers.com All Rights Reserved