Processing Properties Metric English Comments
Pot Life 10 - 20 min
10 - 20 min
Mass: 50g; TM R050-19
Resinlab® EP1225 Black Unfilled Epoxy Adhesive
Resinlab™ EP1225 Black is a two part unfilled epoxy adhesive designed for bonding of metals, ceramics and most plastics. It has slightly thixotropic viscosity to give gap filling ability bust stil..
Pot Life 15 - 20 min
15 - 20 min
Mass: 50g; TM R050-19
Resinlab® EP965 Clear Unfilled Electronic Grade Epoxy Encapsulant
Resinlab™ EP965 Clear is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It cures at room temperature to a tough, semi-rigid polymer. It has good wetting ..
Pot Life 15 - 20 min
15 - 20 min
Mass: 50g; TM R050-19
Resinlab® UR3001HP Black Urethane Encapsulant
Resinlab™ UR3001HP Black is a black, two component, room temperature curing urethane encapsulating system. It is designed to cure completely at room temperature. UR3001HP Black provides excellent e..
Pot Life 10 - 20 min
10 - 20 min
Time before parts must be mated
Lord Adhesives 320 Toughened, High Viscosity SMC, FRP, General Purpose Epoxy Adhesive
Lord Epoxy AdhesivesLord® Epoxy Adhesives create superior bonds for rubber, SMC, plastics and metals. Our epoxy adhesives are widely used in the automotive industry, over 10 million cars and ligh..
Pot Life 15 - 20 min
15 - 20 min
ITW Plexus Plexusâ„¢ MA822 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Designed for structural bonding of metals without primers.Information provided by Illinois Tool Wo..
Pot Life 15 - 20 min
15 - 20 min
100 gm mass
Master Bond EP51FL-1 Rapid Curing Cryogenic Two Component Epoxy
Master Bond Polymer System EP51FL-1 is a two component highly flexible epoxy resin system for high performance bonding sealing and coating. Although most flexiblilized epoxy formulations are very sl..
Pot Life 15 - 20 min
15 - 20 min
100 gram batch
Master Bond EP76M-F Electrically Conductive, Two Part Epoxy
Description: Master Bond EP76M-F is a two component, nickel filled, electrically conductive epoxy system for high performance bonding, sealing, and coating formulated to cure at room temperature or ..
Pot Life 15 - 20 min
15 - 20 min
100 gram mass
Master Bond Supreme 11HT-LO Adhesive and Sealant Serviceable to +400°F
Description: Master Bond Polymer System Supreme 11HT-LO is an easy to use two part epoxy adhesive/sealant combining both high shear and high peel strengths along with a relatively fast cure at room ..
Pot Life 15 - 20 min
15 - 20 min
Loctite® 3951 Gap filling, flexible Urethane Adhesive
Urethane AdhesivesLoctite offers a complete line of one-part and two-part epoxy and urethane adhesives for structural bonding, potting and encapsulating. The Loctite® Durabond® line contains 14 ap..
Pot Life 15 - 20 min

@Temperature 24.0 °C
15 - 20 min

@Temperature 75.2 °F
4 oz. mass
BCC Products BC 6004 Epoxy Surface Coat
BC 6004 is a white thixotropic epoxy surface coat that has the ability to cure and bond to freshly poured wet plaster. This formulated resin compound can be applied with a brush or troweled to a thi..
Pot Life 16 - 20 min

@Temperature 24.0 °C
16 - 20 min

@Temperature 75.2 °F
BCC Products BC 8160 Urethane Casting
BC8160 is a low viscosity two-component urethane casting compound that is specifically formulated for its flexural and impact strength. It is recommended for use for the production casting of highly..
Pot Life 16 - 20 min

@Temperature 24.0 °C
16 - 20 min

@Temperature 75.2 °F
work life
BCC Products BC 8860 Polyurethane Elastomer
BC8860 is a low viscosity two-component urethane casting compound that is specifically formulated for high abrasion and impact resistance. It is recommended for use for the production casting of hig..
Pot Life 18 - 20 min

@Temperature 24.0 °C
18 - 20 min

@Temperature 75.2 °F
BCC Products BC 8870 Polyurethane Elastomer
BC8870 is a low viscosity two-component urethane casting compound that is specifically formulated for high abrasion and impact resistance. It is recommended for use for the production casting of hig..
Pot Life 15 - 20 min
15 - 20 min
Mass: 50g; TM R050-19
Resinlab® EP1195 Flame Retardant Epoxy Casting Resin
Resinlab™ EP1195 is a low viscosity, fast gelling, flame retardant epoxy casting resin system. It is recognized under the Component Recognition Program of Underwriters Laboratories Inc., (File # E1..
Pot Life 15 - 20 min
15 - 20 min
Mass: 50g; TM R050-19
Resinlab® EP965 Black Unfilled Electronic Grade Epoxy Encapsulant
Resinlab™ EP965 Black is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It cures at room temperature to a tough, semi-rigid polymer. It has good wetting ..
Pot Life 15 - 20 min
15 - 20 min
Mass: 50g; TM R050-19
Resinlab® UR3001HP Clear Urethane Encapsulant
Resinlab™ UR3001HP Clear is a clear, two component, room temperature curing urethane encapsulating system. It is designed to cure completely at room temperature. UR3001HP Clear provides excellent e..
Pot Life 10 - 20 min
10 - 20 min
Mass: 100g
Resinlab® UR3005 Clear Two Part Urethane Elastomer
Resinlab™ UR 3005 Clear is a two component, room temperature curing polybutadiene polyurethane casting and potting system. It is designed to cure completely at room temperature. UR 3005 Clear provi..
Pot Life 10 - 20 min
10 - 20 min
Mass: 100g
Resinlab® UR3005 Two Part Urethane Elastomer
Resinlab™ UR 3005 is a two component, room temperature curing polybutadiene polyurethane casting and potting system. It is designed to cure completely at room temperature. UR 3005 provides excellen..