Processing Properties | Metric | English | Comments |
---|---|---|---|
Pot Life | 10 - 15 min | 10 - 15 min | Mass: 50g |
Resinlab® EP1112 Clear Electronic Grade Epoxy Encapsulant Resinlab™ EP 1112 Clear is a two part unfilled fast curing electronic grade epoxy encapsulant designed for small to medium sized castings. It cures completely at room temperature to a tough, flexib.. |
|||
Pot Life | 10 - 20 min | 10 - 20 min | Mass: 50g; TM R050-19 |
Resinlab® EP1225 Black Unfilled Epoxy Adhesive Resinlab™ EP1225 Black is a two part unfilled epoxy adhesive designed for bonding of metals, ceramics and most plastics. It has slightly thixotropic viscosity to give gap filling ability bust stil.. |
|||
Pot Life | 10 - 20 min | 10 - 20 min | Time before parts must be mated |
Lord Adhesives 320 Toughened, High Viscosity SMC, FRP, General Purpose Epoxy Adhesive Lord Epoxy AdhesivesLord® Epoxy Adhesives create superior bonds for rubber, SMC, plastics and metals. Our epoxy adhesives are widely used in the automotive industry, over 10 million cars and ligh.. |
|||
Pot Life | 10 min | 10 min | |
Taiwan PU Corporation PPG CPU-1090C Polyurethane Casting Elastomer A urethane elastomer that can be cured by reacting with a polyamine or a polyolhardener. The molding process is composed of pre-heating, degassing, maxing with a hardener, pouring into the mold, cu.. |
|||
Pot Life | 10 min | 10 min | Curing |
Silikony Polskie Polastosil M-99 Silicone Rubber Rubber with strong hardness |
|||
Pot Life | 10 - 15 min | 10 - 15 min | 100 gram batch |
Master Bond EP41S Fast Curing Epoxy Features Chemical Resistance Description: Master Bond EP41S is a two component epoxy resin compound for durable, high performance, tough, high strength coatings, liners and sealants with outstanding resistance to organic solven.. |
|||
Pot Life | 10 - 15 min | 10 - 15 min | 100 gram mass |
Master Bond EP41SMed Two Component, Low Viscosity, USP Class VI Epoxy System Master Bond Polymer Adhesive EP41S Medical is a two component low viscosity epoxy resin system for high performance bonding, sealing, coating, as well as small encapsulations, pottings and castings... |
|||
Pot Life | 10 min @Temperature 25.0 °C |
10 min @Temperature 77.0 °F |
|
Trelleborg Emerson & Cuming EP679 Patch Paste Blue patch pasteAll information provided by Trelleborg Emerson & Cuming |
|||
Pot Life | 10 min | 10 min | |
Epoxy Technology EPO-TEK® 302 Fast Setting, Optical Epoxy Product Description: EPO-TEK® 302 is a two component, fast-gelling, room temperature curing epoxy, designed for electronic, optical, medical, and general applications. Advantages & Application No.. |
|||
Pot Life | 10 min | 10 min | |
Epoxyset Epoxiohm EO-30FST Electrically Conductive Epoxy Adhesive EO-30-FST is two part, fast cure, silver filled, and high electrical conductivity epoxy adhesive. Both components are silver filled permitting a simple 1:1 mix ratio by weight. It has smooth creamy .. |
|||
Pot Life | 10 - 12 min @Temperature 24.0 °C |
10 - 12 min @Temperature 75.2 °F |
12-14 minutes gel time, ASTM-D-2471, 1/2lb mass |
BCC Products DP-11-88 Urethane Adhesive DP-11-88 is a medium viscosity quick setting easy to use urethane adhesive. This system was specifically designed to bond together the MB2001/MB3000 Model/Tooling Board to create desired dimensions .. |
|||
Pot Life | 10 min | 10 min | |
Tra-Con Tra-Bond FS411 Fast Cure Epoxy Adhesive System TRA-BOND FS-411 is an exceptional epoxy formulation recommended for lower temperature or wet industrial bonding applications where FAST CURING is required. It was designed to have low outgassing in .. |
|||
Pot Life | 10 - 15 min | 10 - 15 min | Mass: 50g |
Resinlab® EP1112 Black Electronic Grade Epoxy Encapsulant Resinlab™ EP 1112 Black is a two part unfilled fast curing electronic grade epoxy encapsulant designed for small to medium sized castings. It cures completely at room temperature to a tough, flexib.. |
|||
Pot Life | 10 min | 10 min | Mass: 50g |
Resinlab® UR3001 Clear Two Part Urethane Encapsulant Resinlab™ UR 3001 is a clear, two component, room temperature curing urethane encapsulating system. It is designed to cure completely at room temperature. UR 3001 provides excellent environmental p.. |
|||
Pot Life | 10 - 20 min | 10 - 20 min | Mass: 100g |
Resinlab® UR3005 Clear Two Part Urethane Elastomer Resinlab™ UR 3005 Clear is a two component, room temperature curing polybutadiene polyurethane casting and potting system. It is designed to cure completely at room temperature. UR 3005 Clear provi.. |
|||
Pot Life | 10 - 20 min | 10 - 20 min | Mass: 100g |
Resinlab® UR3005 Two Part Urethane Elastomer Resinlab™ UR 3005 is a two component, room temperature curing polybutadiene polyurethane casting and potting system. It is designed to cure completely at room temperature. UR 3005 provides excellen.. |
|||
Pot Life | 10 min | 10 min | |
Loctite® Durabond® U-10FL Urethane Adhesive Urethane AdhesivesLoctite offers a complete line of one-part and two-part epoxy and urethane adhesives for structural bonding, potting and encapsulating. The Loctite® Durabond® line contains 14 ap.. |
|||
Pot Life | 10 - 15 min | 10 - 15 min | Mass: 50g; TM R050-19 |
Resinlab® EP1305 Black Highly Toughened Urethane Modified Epoxy Resinlab™ EP1305 Black is a highly toughened urethane modified epoxy designed for bonding PVC, metals, ceramics and other difficult to bond substrates. The system has a thixotropic non-sag viscosi.. |