Polymer Property : Processing Temperature = 421 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Processing Temperature 155 - 216 °C
311 - 421 °F
Average value: 195 °C Grade Count:24
Overview of materials for Thermoplastic Polyurethane, Elastomer, Polyester Grade
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Polyester Grade". Each property range of values reported is minim..
Processing Temperature 193 - 216 °C
379 - 421 °F
adequate mixing to achieve good dispersion
Chevron Phillips Marlex® HHM TR-480Z/M362 Natural high density ethylene hexene copolymer/black concrete  (disc
Benefits: good long term hoop strength performance, very high melt strength, outstanding toughness even at low temperatures, concrete base resinCharacteristics: Pipe Ring ESCR > 2000 h, ASTM F 1248;..
Processing Temperature 194 - 216 °C
381 - 421 °F
Extrusion
Chevron Phillips Marlex® HHM 5502-02 LW High Density Ethylene Hexene Copolymer  (discontinued **)
High Density Ethylene Hexene Copolymer with Synthetic AntistatCustomer Benefits: The resin allows the blow molder to reduce inventory of resin types, because it can be used to package bleach and mos..
Processing Temperature 194 - 216 °C
381 - 421 °F
Extrusion
Chevron Phillips Marlex® HHM 5502-02 LD High Density Ethylene Hexene Copolymer with Antistat  (discontinued **
High Density Ethylene Hexene Copolymer with AntistatCustomer Benefits: The resin allows the blow molder to reduce inventory of resin types, because it can be used to package bleach and most detergen..
Processing Temperature 194 - 216 °C
381 - 421 °F
Extrusion Stock
Chevron Phillips Marlex® HHM 5502-04BN HDPE Hexene Copolymer  (discontinued **)
This resin allows the blow molder to reduce inventory of resin types, because it can be used to package bleach and most detergents. Meets ASTM D4976 - PE 235. ASTM D1248 - Type III, Class A, Cat..
Processing Temperature 193 - 216 °C
379 - 421 °F
Stock Temperature
Chevron Phillips Marlex® HHM TR-140 Polyethylene, Film Grade; HDPE  (discontinued **)
FDA approved.Data provided by the manufacturer
Processing Temperature 193 - 216 °C
379 - 421 °F
Stock Temperature
Chevron Phillips Marlex® HHM TR-144 Polyethylene, Film Grade; HDPE  (discontinued **)
FDA approved.Data provided by the manufacturer
Processing Temperature 193 - 216 °C
379 - 421 °F
adequate mixing to achieve good dispersion
Chevron Phillips Marlex® HHM TR-418N/M358Y Natural medium density ethylene hexene copolymer/yellow concrete  (
Benefits: environmentally-friendly pigment system, yellow color for easy identification, outstanding pipe rind ESCR, UV stabilizer in natural resin, concentrate base resinCharacteristics: Pipe Ring ..
Processing Temperature 188 - 216 °C
370 - 421 °F
Shuman 502 Black Polypropylene Copolymer
Good impact strength, excellent chemical resistance, excellent processability, good wear and abrasion resistance, good resistance to fatigue from flexing.Data provided by the manufacturer.
Processing Temperature 188 - 216 °C
370 - 421 °F
Shuman 502C Black Polypropylene Copolymer
Excellent impact strength, excellent chemical resistance, excellent processability, good wear and abrasion resistance, good resistance to fatigue from flexing.Data provided by the manufacturer.
Processing Temperature 188 - 216 °C
370 - 421 °F
Shuman 510 Black Polypropylene Homopolymer
Excellent chemical resistance, excellent processabilityData provided by the manufacturer.
Processing Temperature 177 - 216 °C
351 - 421 °F
Extrusion
Shuman 710 Utility Black ABS
Good impact strength, easy processability, good chemical resistance, good wear and abrasion resistance.Data provided by the manufacturer.
Processing Temperature 177 - 216 °C
351 - 421 °F
Extrusion
Shuman 720 Black ABS
Good impact strength, easy processability, good chemical resistance, good wear and abrasion resistance.Data provided by the manufacturer.
Processing Temperature 177 - 216 °C
351 - 421 °F
Extrusion
Shuman 780 Grey ABS
Good impact strength, easy processability, good chemical resistance, good wear and abrasion resistance.Data provided by the manufacturer.
Processing Temperature 177 - 216 °C
351 - 421 °F
Extrusion
Shuman 790 Black and Custom Colors ABS-Flame Retardant
Excellent flame retardancy, good impact strength, good chemical resistance, good wear and abrasion resistance.Data provided by the manufacturer.
Processing Temperature 177 - 216 °C
351 - 421 °F
Extrusion
Shuman 791 Black and Custom Colors ABS-Flame Retardant
Long term thermal aging rated. Excellent flame retardancy, good impact strength, good chemical resistance, good wear and abrasion resistance.Data provided by the manufacturer.
Processing Temperature 194 - 216 °C
381 - 421 °F
Extrusion
Chevron Phillips Marlex® HHM 5502 BN High Density Ethylene Hexene-1 Copolymer
High Density Ethylene Hexene-1 CopolymerCustomer Benefits: This resin allows the blow molder to reduce inventory of resin types, because it can be used to package a wide range of products. Has exce..
Processing Temperature 193 - 216 °C
379 - 421 °F
Stock
Chevron Phillips Marlex® HHM TR-418Q MDPE Hexene Copolymer
High performance MDPE resin has been formulated for the demanding requirements of pressure pipe applications. Meets ASTM D4976 PE 225. Meets FDA Regulation 177.1520, suitable for food packaging ap..
Processing Temperature 171 - 216 °C
340 - 421 °F
Blow Molding
Chevron Phillips Marlex® HHM 4903 High Density Ethylene Hexene Copolymer
High Density Ethylene Hexene CopolymerCustomer Benefits: A high performance copolymer that can measure up to the most demanding application. Specifically formulated to provide toughness and durabil..
Processing Temperature 194 - 216 °C
381 - 421 °F
Extrusion
Chevron Phillips Marlex® HHM 4903 High Density Ethylene Hexene Copolymer
High Density Ethylene Hexene CopolymerCustomer Benefits: A high performance copolymer that can measure up to the most demanding application. Specifically formulated to provide toughness and durabil..
Processing Temperature 194 - 216 °C
381 - 421 °F
Extrusion
Chevron Phillips Marlex® HHM 5202 BN High Density Ethylene Hexene-1 Copolymer
High Density Ethylene Hexene-1 CopolymerCustomer Benefits: For the blow molder who wants to stock one resin that will be suitable for most of his customers' packaging needs. Lightweight containers ..
Processing Temperature 194 - 216 °C
381 - 421 °F
Extrusion
Chevron Phillips Marlex® HHM 5202-02 BN High Density Ethylene Hexene-1 Copolymer
High Density Ethylene Hexene-1 CopolymerCustomer Benefits: For the blow molder who wants to stock one resin that will be suitable for most of his customers' packaging needs. Lightweight containers ..
Processing Temperature 194 - 216 °C
381 - 421 °F
Extrusion
Chevron Phillips Marlex® HHM 5502 LD High Density Ethylene Hexene Copolymer with Antistat
High Density Ethylene Hexene Copolymer with AntistatCustomer Benefits: This resin allows the blow molder to reduce inventory of resin types, because it can be used to package a wide range of product..
Processing Temperature 199 - 216 °C
390 - 421 °F
Optimum Extrusion Temperature
Dow PELLETHANE® 2355-55DE Polyurethane Elastomer, Polyester Polyadipate Based  (discontinued **)
Description: PELLETHANE® 2355-55DE polyester polyadipate based polyurethane elastomer has excellent oil and chemical resistance. Applications include: Film, Sheet, Tubing, Recreation and sporting e..