Total PPC M6823MZ Metallocene Isostatic Propylene Polymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Total Atofina
Trade Name PPC
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total PPC M6823MZ Metallocene Isostatic Propylene Polymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TOTAL Petrochemicals Polypropylene M6823MZ is an isostatic form of copolymer polypropylene made via TOTAL Petrochemicals proprietary metallocene catalyst technology.Clarity. M6823MZ incorporates the latest generation of clarification technology resulting in excellent cycle time and superior performances in thin-wall, multi-cavity molds.FDA. M6823MZ complies with FDA regulations Title 21 CFR Section 177.1520 (c) 3.1 and may be used under these provisions for food contact and packaging.Recommended Applications. M6823MZ is a medium molecular weight material recommended for injection molding. However, due to its unique and interesting properties, other applications may exist.Information provided by Total Petrochemicals.
Physical Properties Metric English Comments
Melt Flow 30 g/10 min
30 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 29.0 MPa
4210 psi
ASTM D638
Elongation at Yield 12 %
12 %
ASTM D638
Tensile Modulus 1.24 GPa
180 ksi
ASTM D638
Flexural Modulus 1.19 GPa
173 ksi
ASTM D790
Izod Impact, Notched 0.370 J/cm
0.693 ft-lb/in
ASTM D256
Impact Test 16.5 J

@Thickness 3.17 mm
12.2 ft-lb

@Thickness 0.125 in
Drop Impact; API
Thermal Properties Metric English Comments
Melting Point 136 °C
277 °F
DSC
Deflection Temperature at 0.46 MPa (66 psi) 89.0 °C
192 °F
ASTM D648
Optical Properties Metric English Comments
Haze 6.0 %

@Thickness 1.02 mm
6.0 %

@Thickness 0.0400 in
ASTM D1003
Processing Properties Metric English Comments
Processing Temperature 199 - 249 °C
390 - 480 °F