Polymer Property : Processing Temperature = 415 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Processing Temperature 196 - 213 °C
385 - 415 °F
Average value: 205 °C Grade Count:5
Overview of materials for PVC, High Impact
This property data is a summary of similar materials in the MatWeb database for the category "PVC, High Impact". Each property range of values reported is minimum and maximum values of appropriate M..
Processing Temperature 199 - 213 °C
390 - 415 °F
Average value: 207 °C Grade Count:3
Overview of materials for PVC, Transparent
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Transparent". Each property range of values reported is minimum and maximum values of appropriate M..
Copyright © lookpolymers.com All Rights Reserved