Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
Cavity temperature
Celanese Celanex® 1462Z PBT, 30% Glass Reinforced  (Unverified Data**)
Celanex 1462Z is a general purpose, 30% glass reinforced polybutylene terephthalate with a good balance of mechanical properties and processability.30% glass-fiber, general purposeInformation provid..
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
Cavity temperature
Celanese Celanex® 1602Z PBT  (Unverified Data**)
Celanex 1602Z is a general purpose, unreinforced polybutylene terephthalate with a good balance of mechanical properties and processability. Celanex 1602Z has an internal lubricant.Lubricated extrus..
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
Cavity temperature
Celanese Celanex® 1632Z PBT, 15% Glass Reinforced  (Unverified Data**)
Celanex 1632Z is a general purpose, 15% fiberglass reinforced polybutylene terephthalate with a good balance of mechanical properties and processability.15% glass-fiber, improved impactInformation p..
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
Cavity temperature
Celanese Celanex® 2404 MT PBT, Medical Technology  (Unverified Data**)
Celanex 2404 MT Natural is an unreinforced PTFE filled PBT with improved friction, sliding, and wear properties that complies with the requirements of CFR 21 177.1660 of the Food and Drug Administra..
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
Cavity temperature
Celanese Celanex® 3300 PBT, 30% Glass Reinforced  (Unverified Data**)
Ceanex 3300 is a general purpose, 30% glass reinforced, polybutylene terephthalate that offers a superior combination of mechanical, electrical, and thermal properties. This grade provides outstandi..
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
Cavity temperature
Celanese Celanex® 6400-2 PBT, Mineral / Glass Reinforced  (Unverified Data**)
40% glass/mineral reinforced polyester, providing warp resistance and improved surface finish.40% glass/mineral filled, low warpInformation provided by Celanese
Processing Temperature 65.0 - 96.0 °C
149 - 205 °F
Cavity temperature
Celanese Celanex® 6500 PBT, 30% Mineral / Glass Reinforced  (Unverified Data**)
Celanex 6500 is a 30% glass/mineral polyester with improved surface finish and a good balance of mechanical properties and processability.30% glass/mineral, low warpInformation provided by Celanese
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
Cavity temperature
Celanese Celanex® MT2008 PBT  (Unverified Data**)
Celanex MT2008 is a medical grade unreinforced polybutylene terephthalate with a good balance of mechanical properties and processability for use in melt blown applications.Unfilled PBT for medical ..
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
cavity
Celanese CELANEX 1632Z PBT, 15% Glass Reinforced
Celanex 1632Z is a general purpose, 15% fiberglass reinforced polybutylene terephthalate with a good balance of mechanical properties and processability.Information provided by Celanese
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
cavity
Celanese CELANEX 1700A PBT, Unfilled
Celanex 1700A is a very high molecular weight grade of unreinforce polybutylene terephthalate for extrusion applications.Information provided by Celanese
Processing Temperature 65.0 - 96.0 °C
149 - 205 °F
cavity
Celanese CELANEX 2002-3 PBT, Unfilled
Celanex 2002-3 is a general purpose, unreinforced polybutylene terephthalate with a good balance of mechanical properties and processability. Celanex 2002-3 is a medium flow material that contains ..
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
cavity
Celanese CELANEX 2003HR PBT, Unfilled
Celanex 2003HR is an unfilled polybutylene terephthalate which has an excellent hydrolysis resistance, mechanical properties and processabilityInformation provided by Celanese
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
cavity
Celanese CELANEX 3200-2FC PBT, 15% Glass Reinforced
Celanex 3200-2FC is a general purpose, 15% glass reinforced polybutylene terephthalate with a good balance of mechanical properties and processability for use in food contact applications. Celanex 3..
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
cavity
Celanese CELANEX 3300D PBT, 30% Glass Reinforced
Celanex 3300D is a general purpose, 30% glass reinforced, polybutylene terephthalate that offers a superior combination of mechanical, electrical, and thermal properties. This grade provides outsta..
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
cavity
Celanese CELANEX 3300FC PBT, 30% Glass Reinforced
Celanex 3300FC is a general purpose, 30% glass reinforced, polybutylene terephthalate that offers a superior combination of mechanical, electrical, and thermal properties. This grade provides outsta..
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
cavity
Celanese CELANEX 3309HRHF PBT, 30% Glass Reinforced
Celanex 3309HRHF is a 30% fiberglass reinforced Polybutylene Terephthalate which has excellent hydrolysis resistance, mechanical properties and improved flow.Information provided by Celanese
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
cavity
Celanese CELANEX 3309HRLM PBT, 30% Glass Reinforced
Celanex 3309HRLM is a non-lubricated, 30% fiberglass reinforced Polybutylene Terephthalate which has excellent hydrolysis resistance, mechanical properties and processability. lIt is a asermarkable ..
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
cavity
Celanese CELANEX 4309AR PBT
Celanex 4309AR is a 30% glass reinforced PBT with enhanced resistance to hydrolysis, alkaline environments and salt water spray.Information provided by Celanese
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
cavity
Celanese CELANEX 5200-2 PBT, 15% Glass Reinforced
Celanex 5200-2 is a 15% fiberglass reinforced polyester with improved surface finish. Celanex 5200-2 contains an internal lubricant.Information provided by Celanese
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
cavity
Celanese Celanex® 2003-2 PBT, Unfilled
Celanex 2003-2 is a general purpose, unreinforced polybutylene terephthalate with a good balance of mechanical properties, processability, and good flow characterictics. Celanex 2003-2 is a medium h..
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
cavity
Celanese Celanex® 3226 PBT, Glass Reinforced
Celanex 3226 is a non-exuding, 20% glass-filled, flame retarded polybutylene terephthalate (PBT) which has an excellent balance of mechanical properties and processability. It is well suited for ele..
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
cavity
Celanese Celanex® 4302HS PBT, 30% Glass Reinforced
Celanex 4302HS is a 30% glass reinforced PBT designed for improved mold flow, warp resistance and surface appearance. Celanex 4302HS is ideally suited for heat shock applications such as ignition co..
Processing Temperature 65.0 - 96.0 °C
149 - 205 °F
cavity
Celanese Celanex® 7316 PBT, 35% Mineral / Glass Reinforced
Celanex 7316 is a non-exuding (UL and CSA approved V-0 at 1/32 inch), 35% glass/mineral reinforced PBT, which has an excellent balance of mechanical properties and processability. It is well suited..
Processing Temperature 65.0 - 96.0 °C
149 - 205 °F
cavity
Celanese VANDAR 4612R PBT, 7% Glass Reinforced
Vandar 4612R is a high impact polyester alloy containing 7% glass. It possesses excellent impact properties as well as toughness and moldability. Dimensional stability, chemical resistance, and low ..
Processing Temperature 65.0 °C
149 °F
Cure 1 hrs
Aptek 2710A/B Low modulus silicone adhesive
Low modulus silicone adhesive; -110ºC to 260ºC operating range; Low outgassing/space grade; Electrostatically Discharging (ESD)APTEK 2710-A/B is a two component, black, low modulus, thixotropic, s..
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
cavity
Celanese CELANEX 3300-2FC PBT, 30% Glass Reinforced
Celanex 3300-2FC is a general purpose, 30% glass reinforced, polybutylene terephthalate that offers a superior combination of mechanical, electrical, and thermal properties. This grade provides outs..
Processing Temperature 65.0 - 96.0 °C
149 - 205 °F
cavity
Celanese VANDAR 2100 PBT, Unfilled
Vandar 2100 is a polyester alloy designed to offer maximum impact strength at room and low temperatures. This unfilled compound is characterized by outstanding chemical resistance, dimensional stabi..
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
Cavity temperature
Celanese Celanex® 1600FC PBT  (Unverified Data**)
Celanex 1600FC is a high molecular weight grade of unreinforced polybutylene terephthalate for use in food contact applications that can be used in both extrusion and injection molding applications...
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
Cavity temperature
Celanese Celanex® 3300D PBT, 30% Glass Reinforced  (Unverified Data**)
Celanex 3300D is a general purpose, 30% glass reinforced, polybutylene terephthalate that offers a superior combination of mechanical, electrical, and thermal properties. This grade provides outsta..
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
Cavity temperature
Celanese Celanex® 3309HRT PBT, 30% Glass Reinforced  (Unverified Data**)
Celanex 3309HRT is a non-lubricated, 30% fiberglass reinforced Polybutylene Terephthalate that has excellent hydrolysis resistance, toughness and improved flow.30% glass reinforced, unlubricated, hy..