Material Notes:
Processing: 100/80 pbw; Potlife: 6-7 days/20°C (68°F), 12-24 h/40°C (105°F), 0.75-7 h /60°C (140°F); mix at 50-80°C (120-175°F); cures in: 1 h/100°C (212°F) + 4 h/150°C (300°F) postcure.Applications: Potting, impregnating and laminating.
Physical Properties Metric English Comments
Density 1.23 g/cc
0.0444 lb/in³
Water Absorption 0.25 - 0.30 %
0.25 - 0.30 %
(60x10X4 mm bar) after 10 days at 20°C (77°F)
0.25 - 0.30 %
0.25 - 0.30 %
(60x10X4 mm bar) after 1 hour at 100°C (212°F)
Viscosity 50 - 150 cP

@Temperature 60.0 °C
50 - 150 cP

@Temperature 140 °F
200 - 400 cP

@Temperature 40.0 °C
200 - 400 cP

@Temperature 104 °F
1000 - 2000 cP

@Temperature 25.0 °C
1000 - 2000 cP

@Temperature 77.0 °F
Vapor Pressure <= 0.0000133 bar

@Temperature 20.0 °C
<= 0.0100 torr

@Temperature 68.0 °F
AboCure
0.000933 bar

@Temperature 80.0 °C
0.700 torr

@Temperature 176 °F
AboCure
<= 0.00133 bar

@Temperature 180 °C
<= 1.00 torr

@Temperature 356 °F
AboCast
0.00267 bar

@Temperature 120 °C
2.00 torr

@Temperature 248 °F
AboCure
0.0213 bar

@Temperature 135 °C
16.0 torr

@Temperature 275 °F
AboCure
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 75.84 MPa
11000 psi
Modulus of Elasticity 2.758 GPa
400.0 ksi
Flexural Yield Strength 137.9 MPa
20000 psi
Compressive Yield Strength 124.1 MPa
18000 psi
Thermal Properties Metric English Comments
CTE, linear 55.0 - 65.0 µm/m-°C

@Temperature 20.0 °C
30.6 - 36.1 µin/in-°F

@Temperature 68.0 °F
Maximum Service Temperature, Air 130 °C
266 °F
Deflection temperature; load unknown.
Electrical Properties Metric English Comments
Electrical Resistivity >= 1.50e+16 ohm-cm
>= 1.50e+16 ohm-cm
Dielectric Constant 3.0 - 3.3

@Frequency 1e+6 Hz
3.0 - 3.3

@Frequency 1e+6 Hz
3.2 - 3.5

@Frequency 1000 Hz
3.2 - 3.5

@Frequency 1000 Hz
3.4 - 3.7

@Frequency 50 Hz
3.4 - 3.7

@Frequency 50 Hz
Dielectric Strength 13.78 - 15.75 kV/mm

@Thickness 3.17 mm
350.0 - 400.0 kV/in

@Thickness 0.125 in
Short time value
Dissipation Factor 0.0050 - 0.010

@Frequency 50 Hz
0.0050 - 0.010

@Frequency 50 Hz
0.0050 - 0.010

@Frequency 1000 Hz
0.0050 - 0.010

@Frequency 1000 Hz
0.015 - 0.020

@Frequency 1e+6 Hz
0.015 - 0.020

@Frequency 1e+6 Hz
Processing Properties Metric English Comments
Processing Temperature 50.0 - 80.0 °C
122 - 176 °F
Pot Life 45.0 - 420 min

@Temperature 60.0 °C
45.0 - 420 min

@Temperature 140 °F
720 - 1440 min

@Temperature 40.0 °C
720 - 1440 min

@Temperature 104 °F
8640 - 10080 min

@Temperature 20.0 °C
8640 - 10080 min

@Temperature 68.0 °F