Processing Properties Metric English Comments
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
Cavity temperature
Celanese Celanex® 1700A PBT  (Unverified Data**)
Celanex 1700A is a very high molecular weight grade of unreinforce polybutylene terephthalate for extrusion applications.Highest molecular weightInformation provided by Celanese
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
Cavity temperature
Celanese Celanex® 2001 PBT  (Unverified Data**)
Celanex 2001 is an unreinforced polybutylene terephthalate resin with improved hydrolysis resistance developed for use in fiber optic buffer tube applications. Celanex 2001 exhibits the high melt st..
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
Cavity temperature
Celanese Celanex® 2016 PBT  (Unverified Data**)
Celanex 2016 is a non-exuding flame retarded (UL and CSA approved V-0 at 1/32 inch and 5V at 1/8 inch), unreinforced polybutylene terephthalate which has an excellent balance of mechanical propertie..
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
Cavity temperature
Celanese Celanex® 2404 MT PBT, Medical Technology  (Unverified Data**)
Celanex 2404 MT Natural is an unreinforced PTFE filled PBT with improved friction, sliding, and wear properties that complies with the requirements of CFR 21 177.1660 of the Food and Drug Administra..
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
Cavity temperature
Celanese Celanex® 3200-2 PBT, 15% Glass Reinforced  (Unverified Data**)
Celanex 3200-2 is a general purpose, 15% glass reinforced polybutylene terephthalate with a good balance of mechanical properties and processability. Celanex 3200-2 contains an internal lubricant.15..
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
Cavity temperature
Celanese Celanex® 3300-2LM PBT, Glass Reinforced  (Unverified Data**)
Celanex 3300-2LM is a 30% glass-filled PBT that is enhanced for improved laser marking graphics. It contains an internal lubricant for enhanced mold release.30% glass-filled PBT, laser markableInfo..
Processing Temperature 65.0 - 96.0 °C
149 - 205 °F
Cavity temperature
Celanese Celanex® 3400-2 PBT, 40% Glass Reinforced  (Unverified Data**)
Celanex 3400-2 is a general purpose, 40% glass reinforced polybutylene terephthalate that offers a good combination of mechanical, electrical, and thermal properties. This grade provides outstanding..
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
Cavity temperature
Celanese Celanex® 4300FC PBT, 30% Glass Reinforced  (Unverified Data**)
Celanex 4300FC is a toughened, 30% glass reinforced PBT for use in food contact applications.30% glass reinforced PBT for use in food contact applicationsInformation provided by Celanese
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
Cavity temperature
Celanese Celanex® 5200-2 PBT, 15% Glass Reinforced  (Unverified Data**)
Celanex 5200-2 is a 15% fiberglass reinforced polyester with improved surface finish. Celanex 5200-2 contains an internal lubricant.15% glass reinforced, high gloss, general purpose, lubricatedInfor..
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
Cavity temperature
Celanese Celanex® 531HS PBT, Glass Reinforced  (Unverified Data**)
Celanex 531HS is a 30% fiberglass reinforced PBT which has an excellent balance of mechanical properties and processability. Celanex 531HS is specifically designed to exhibit excellent thermal shoc..
Processing Temperature 65.0 - 96.0 °C
149 - 205 °F
Cavity temperature
Celanese Celanex® 6500 PBT, 30% Mineral / Glass Reinforced  (Unverified Data**)
Celanex 6500 is a 30% glass/mineral polyester with improved surface finish and a good balance of mechanical properties and processability.30% glass/mineral, low warpInformation provided by Celanese
Processing Temperature 65.0 - 96.0 °C
149 - 205 °F
Cavity temperature
Celanese Vandar® 2500 PBT  (Unverified Data**)
Vandar 2500 is an unfilled polyester alloy which exhibits excellent toughness and impact strength. It is specially designed to offer excellent chemical resistance, good colorability and dimensional ..
Processing Temperature 65.0 - 70.0 °C
149 - 158 °F
Temperature setting, A component
Taiwan PU Corporation TPL-THANE 5085-A/B High Pressure Urethane Spraying Elastomer
5085-A is a high reactivity polyethamine content extender. 5085-B is a methylene diphenyklene dissocyanate(MDI). They make up the third generation high pressure urethane spraying elastomer. It ha..
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
cavity
Celanese CELANEX 1602Z PBT, Unfilled
Celanex 1602Z is a general purpose, unreinforced polybutylene terephthalate with a good balance of mechanical properties and processability. Celanex 1602Z has an internal lubricant.Information provi..
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
cavity
Celanese CELANEX 2001 PBT, Unfilled
Celanex 2001 is an unreinforced polybutylene terephthalate resin with improved hydrolysis resistance developed for use in fiber optic buffer tube applications. Celanex 2001 exhibits the high melt st..
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
cavity
Celanese CELANEX 2001FC PBT, Unfilled
Celanex 2001FC is an unreinforced polybutylene terephthalate resin with improved hydrolysis resistance developed for use in fiber optic buffer tube applications for use in food contact applications...
Processing Temperature 65.0 - 96.0 °C
149 - 205 °F
cavity
Celanese CELANEX 2002-3 PBT, Unfilled
Celanex 2002-3 is a general purpose, unreinforced polybutylene terephthalate with a good balance of mechanical properties and processability. Celanex 2002-3 is a medium flow material that contains ..
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
cavity
Celanese CELANEX 3200-2 PBT, 15% Glass Reinforced
Celanex 3200-2 is a general purpose, 15% glass reinforced polybutylene terephthalate with a good balance of mechanical properties and processability. Celanex 3200-2 contains an internal lubricant.In..
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
cavity
Celanese CELANEX 3300D PBT, 30% Glass Reinforced
Celanex 3300D is a general purpose, 30% glass reinforced, polybutylene terephthalate that offers a superior combination of mechanical, electrical, and thermal properties. This grade provides outsta..
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
cavity
Celanese CELANEX 3300LM PBT, 30% Glass Reinforced
Celanex 3300LM is a 30% glass reinforced lasermarkable grade specially formulated to yield crisp marks when subjected to a Nd:YAG laser or equivalent operated at 1064nm or 532nm. Lasers operating i..
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
cavity
Celanese CELANEX 4300 PBT, 30% Glass Reinforced
Celanex 4300 is a toughened, 30% glass reinforced PBT.Information provided by Celanese
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
cavity
Celanese CELANEX 4300FC PBT, 30% Glass Reinforced
Celanex 4300FC is a toughened, 30% glass reinforced PBT for use in food contact applications.Information provided by Celanese
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
cavity
Celanese CELANEX MT2008 PBT, Unfilled
Celanex MT2008 is a medical grade unreinforced polybutylene terephthalate with a good balance of mechanical properties and processability for use in melt blown applications.Information provided by C..
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
cavity
Celanese Celanex® 3200 PBT, 15% Glass Reinforced
Celanex 3200 is a general purpose, 15% glass reinforced polybutylene terephthalate with a good balance of mechanical properties and processability.To avoid hydrolytic degradation during processing, ..
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
cavity
Celanese Celanex® 4302HS PBT, 30% Glass Reinforced
Celanex 4302HS is a 30% glass reinforced PBT designed for improved mold flow, warp resistance and surface appearance. Celanex 4302HS is ideally suited for heat shock applications such as ignition co..
Processing Temperature 65.0 - 96.0 °C
149 - 205 °F
cavity
Celanese VANDAR 2100UV PBT, Impact Modified
Vandar 2100UV is a polyester alloy designed to offer maximum impact strength at room and low temperatures. This unfilled compound is characterized by outstanding chemical resistance, dimensional sta..
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
cavity
Celanese CELANEX 3300-2FC PBT, 30% Glass Reinforced
Celanex 3300-2FC is a general purpose, 30% glass reinforced, polybutylene terephthalate that offers a superior combination of mechanical, electrical, and thermal properties. This grade provides outs..
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
cavity
Celanese Celanex® 3318 PBT, 30% Glass Reinforced
Celanex 3318 is a non-exuding (UL approved V-0 at 1/64 inch), 30% fiberglass reinforced polybutylene terephthalate which has an excellent balance of mechanical properties and processability. It is w..
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
Cavity temperature
Celanese Celanex® 2002-2 PBT  (Unverified Data**)
Celanex 2002-2 is a general purpose, unreinforced polybutylene terephthalate with a good balance of mechanical properties and processability. Celanex 2002-2 ia a medium flow material that contains a..
Processing Temperature 65.0 - 96.0 °C
149 - 205 °F
cavity
Celanese VANDAR 4662Z PBT, 30% Glass Reinforced
Vandar 4662Zis a high impact polyester alloy which contains 30% glass fiber loading. It is characterized by toughness, dimensional stability, and high modulus. Good weatherability and moldability ar..
Copyright © lookpolymers.com All Rights Reserved