Skamol Group VIP 12 Vermiculite Insulating Slab

Category Ceramic , Oxide , Silicon Oxide
Manufacturer Skamol Group
Trade Name VIP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Skamol Group VIP 12 Vermiculite Insulating Slab.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
SKAMOL V-1100 & VIP-12 vermiculite slabs have the following characteristics: Max. service temperature: Up to 1150°C (2102°F)Hot-face applications or back-up insulation of all refractory constructionsExcellent insulating valueHigh mechanical strengthGood thermal shock resistanceCan be used in furnaces with reducing atmospheres due to their high resistance to carbon monoxide and hydrocarbonsSeveral grades available in various combinations of bulk density, insulation properties and compressive strengthA variety of uses in high-temperature kilns and furnaces, combustion plants, boilers as well as in hearth and heating appliancesHigh-density grade VIP-12 has a good resistance to cryolite and fluorides, which makes it particularly suitable for uses within the primary aluminum industry.Information provided by Skamol.
Physical Properties Metric English Comments
Bulk Density 1.20 g/cc
0.0434 lb/in³
Dry
Loss On Ignition 4.00 %

@Temperature 1025 °C
4.00 %

@Temperature 1877 °F
Porosity 55 %
55 %
Total
Mechanical Properties Metric English Comments
Modulus of Rupture 0.00360 GPa
0.522 ksi
EN 993-6: 1995
Compressive Strength 11.0 MPa
1600 psi
EN 1094-5: 1995
Thermal Properties Metric English Comments
CTE, linear 12.0 µm/m-°C

@Temperature 20.0 - 750 °C
6.67 µin/in-°F

@Temperature 68.0 - 1380 °F
BS 1902: section 5.3: 1990
Specific Heat Capacity 1.10 J/g-°C
0.263 BTU/lb-°F
Thermal Conductivity 0.230 W/m-K

@Temperature 200 °C
1.60 BTU-in/hr-ft²-°F

@Temperature 392 °F
Mean temp.; ASTM C-182
0.260 W/m-K

@Temperature 400 °C
1.80 BTU-in/hr-ft²-°F

@Temperature 752 °F
ASTM C-182
0.290 W/m-K

@Temperature 600 °C
2.01 BTU-in/hr-ft²-°F

@Temperature 1110 °F
ASTM C-182
0.330 W/m-K

@Temperature 800 °C
2.29 BTU-in/hr-ft²-°F

@Temperature 1470 °F
ASTM C-182
Maximum Service Temperature, Air 1150 °C
2100 °F
Component Elements Properties Metric English Comments
Al2O3 20 %
20 %
CaO 1.0 %
1.0 %
Fe2O3 3.0 %
3.0 %
K2O 7.0 %
7.0 %
MgO 10 %
10 %
Na2O 0.10 %
0.10 %
SiO2 51 %
51 %
TiO2 1.0 %
1.0 %
Descriptive Properties Value Comments
Color Light Brown
Pyrometric Cone Equivalent 1221°C
ASTM C24-89, ORTON cones
Resistance to Thermal Shock Min 30 cycles
EN 993-11: 1998, heating to 950°C (1742°F)