Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.140 W/m-K @Temperature 23.9 °C |
0.972 BTU-in/hr-ft²-°F @Temperature 75.0 °F |
|
Paratherm Corporation Paratherm™ CR Heat Transfer Fluid Paratherm CR® heat transfer fluid is a blend of synthetic components formulated to provide superior cooling performance in closed-loop heat-transfer systems operating down to -88°C (-127°F) yet i.. |
|||
Thermal Conductivity | 0.140 W/m-K @Temperature 870 °C |
0.972 BTU-in/hr-ft²-°F @Temperature 1600 °F |
|
Pyrotek M-13 Compressible/Insulating Boards ApplicationsHigh temperature gaskets Non-conductive insulation Lid gaskets AdvantagesDurable Resistant to chemical attack Excellent mechanical strength Low air permeability Information provided by P.. |
|||
Thermal Conductivity | 0.140 W/m-K @Temperature 1100 °C |
0.972 BTU-in/hr-ft²-°F @Temperature 2010 °F |
|
Zircar Zirconia ZYFB-3 Zirconia Boards, Discs, and Cylinders Insulation Type ZYFB Boards, Discs and Cylinders are rigid, refractory structures composed of yttria-stabilized zirconia fibers that do not undergo the usual phase transitions associated with pure zirconia. Ty.. |
|||
Thermal Conductivity | 0.140 W/m-K @Temperature 1100 °C |
0.972 BTU-in/hr-ft²-°F @Temperature 2010 °F |
|
Zircar Zirconia ZYZ-3 Zirconia Boards and Discs Insulation Type ZYZ Boards and Discs are rigid, refractory structures composed of yttria-stabilized zirconia fibers that are bonded with silica. This unique composition provides Type ZYZ insulation with the lo.. |
|||
Thermal Conductivity | 0.140 - 0.220 W/m-K @Temperature 100 °C |
0.972 - 1.53 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast GOLITE 95 Refractory Insulating Castable Description: Golite 95 is widely applied as an insulating backlining behind a dense castable, especially in the petrochemical industry.Remarks: These values apply to cast products. Also available in.. |
|||
Thermal Conductivity | 0.140 W/m-K @Temperature 600 °C |
0.972 BTU-in/hr-ft²-°F @Temperature 1110 °F |
ASTMÂ C-182 |
Skamol Group ISOPERLOR 550P Perlite Insulating Brick & Block ISOPERLOR perlite insulating bricks & blocks have the following characteristics: Max. service temperature 900°C (1652°F)Back-up insulation onlyExcellent insulating propertiesVery lightweight a.. |
|||
Thermal Conductivity | 0.140 W/m-K @Temperature 400 °C |
0.972 BTU-in/hr-ft²-°F @Temperature 752 °F |
ASTMÂ C-182 |
Skamol Group Moler SUPRA Insulating Block SKAMOL Moler insulating bricks & blocks have the following characteristics: Max. service temperature: Up to 1000°C (1832°F)Back-up insulation Excellent insulating propertiesHigh mechanical str.. |
|||
Thermal Conductivity | 0.140 W/m-K @Temperature 200 °C |
0.972 BTU-in/hr-ft²-°F @Temperature 392 °F |
Mean temp.; ASTMÂ C-182 |
Skamol Group SKAMOLEX V-1100 (475) Customized Shape SKAMOLEX customized shapes have the following characteristics: Max. service temperature: Up to 1150°C (2102°F)Hot-face applications or back-up insulationA large variety of specialized and vers.. |
|||
Thermal Conductivity | 0.140 W/m-K @Temperature 400 °C |
0.972 BTU-in/hr-ft²-°F @Temperature 752 °F |
ASTMÂ C-182 |
Skamol Group V-1100 375 Vermiculite Insulating Slab SKAMOL V-1100 & VIP-12 vermiculite slabs have the following characteristics: Max. service temperature: Up to 1150°C (2102°F)Hot-face applications or back-up insulation of all refractory constr.. |
|||
Thermal Conductivity | 0.140 W/m-K @Temperature 200 °C |
0.972 BTU-in/hr-ft²-°F @Temperature 392 °F |
Mean temp.; ASTMÂ C-182 |
Skamol Group V-1100 475 Vermiculite Insulating Slab SKAMOL V-1100 & VIP-12 vermiculite slabs have the following characteristics: Max. service temperature: Up to 1150°C (2102°F)Hot-face applications or back-up insulation of all refractory constr.. |
|||
Thermal Conductivity | 0.140 W/m-K @Temperature 400 °C |
0.972 BTU-in/hr-ft²-°F @Temperature 752 °F |
ASTMÂ C-182 |
Skamol Group V-LITE 375 Vermiculite Insulating Brick V-LITE vermiculite insulating bricks have the following characteristics: Max. service temperature 1100°C (2012°F)Hot-face applications and back-up insulationGood insulation valueHigh mechanica.. |
|||
Thermal Conductivity | 0.140 W/m-K @Temperature 200 °C |
0.972 BTU-in/hr-ft²-°F @Temperature 392 °F |
Mean temp.; ASTMÂ C-182 |
Skamol Group V-LITE 475 Vermiculite Insulating Brick V-LITE vermiculite insulating bricks have the following characteristics: Max. service temperature 1100°C (2012°F)Hot-face applications and back-up insulationGood insulation valueHigh mechanica.. |
|||
Thermal Conductivity | 0.140 W/m-K @Temperature 800 °C |
0.972 BTU-in/hr-ft²-°F @Temperature 1470 °F |
|
Zircar Ceramics AXHTM Alumina-Silica Insulation ZIRCAR Alumina Silica Insulation Type AXL and Type AXHTM are inorganically bound insulation boards typified by their rigid outer surfaces and unbound interiors. They offer low thermal conductivity a.. |
|||
Thermal Conductivity | 0.140 W/m-K @Temperature 1100 °C |
0.972 BTU-in/hr-ft²-°F @Temperature 2010 °F |
|
Zircar Zirconia ZYC Zirconia Cylinders Insulation Zircar Zirconia Cylinders Type ZYC are rigid, free standing refractory structures composed of yttria stabilized zirconia fibers that are bonded with silica. The material is evenly bonded, allowing .. |
|||
Thermal Conductivity | 0.140 W/m-K @Temperature 1100 °C |
0.972 BTU-in/hr-ft²-°F @Temperature 2010 °F |
|
Zircar Zirconia ZYFB-3 Zirconia Boards, Discs, and Cylinders Insulation Type ZYFB Boards, Discs and Cylinders are rigid, refractory structures composed of yttria-stabilized zirconia fibers that do not undergo the usual phase transitions associated with pure zirconia. Ty.. |
|||
Thermal Conductivity | 0.140 W/m-K @Temperature 1100 °C |
0.972 BTU-in/hr-ft²-°F @Temperature 2010 °F |
|
Zircar Zirconia ZYZ-3 Zirconia Boards and Discs Insulation Type ZYZ Boards and Discs are rigid, refractory structures composed of yttria-stabilized zirconia fibers that are bonded with silica. This unique composition provides Type ZYZ insulation with the lo.. |
|||
Thermal Conductivity | 0.140 W/m-K @Temperature 871 °C |
0.972 BTU-in/hr-ft²-°F @Temperature 1600 °F |
|
Zircar Refractory Composites ASPA-880 Alumina-Silica Fiber Paper ASPA-880 is a high temperature, lightweight refractory material made from alumina-silica fibers formed into highly flexible sheets. It is made from shorter and smaller diameter fibers with a higher .. |
|||
Thermal Conductivity | 0.140 W/m-K @Temperature 871 °C |
0.972 BTU-in/hr-ft²-°F @Temperature 1600 °F |
|
Zircar Refractory Composites ASPA-970 Alumina-Silica Fiber Paper ASPA-970 is an industrial grade, lightweight refractory material made from alumina-silica fibers formed into highly flexible sheets. This alumina-silica fiber paper exhibits very low thermal conduct.. |
|||
Thermal Conductivity | 0.140 W/m-K @Temperature 37.8 °C |
0.972 BTU-in/hr-ft²-°F @Temperature 100 °F |
|
Duratherm 600 Paraffinic Heat Transfer Fluid Duratherm 600 - thermal fluid rated to 600°F it contains the industries most aggressive blend of additives for long, trouble free operation in a variety of applications. Specifically engineered to .. |
|||
Thermal Conductivity | 0.140 W/m-K @Temperature 260 °C |
0.972 BTU-in/hr-ft²-°F @Temperature 500 °F |
ASTM C182 |
BNZ Materials BNZ-23 Insulating Firebrick BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Thermal Conductivity | 0.140 W/m-K @Temperature 204 °C |
0.972 BTU-in/hr-ft²-°F @Temperature 399 °F |
|
BNZ Materials Marinite® C Ceramic Board for Aluminum Contact These boards are heat treated formulations for use in conveying, containing and forming molten aluminum and other non-ferrous metals. Applications include holding furnace linings, tips for continuou.. |
|||
Thermal Conductivity | 0.140 W/m-K @Temperature 316 °C |
0.972 BTU-in/hr-ft²-°F @Temperature 601 °F |
|
BNZ Materials Marinite® C Ceramic Board for Aluminum Contact These boards are heat treated formulations for use in conveying, containing and forming molten aluminum and other non-ferrous metals. Applications include holding furnace linings, tips for continuou.. |
|||
Thermal Conductivity | 0.140 W/m-K @Temperature 482 °C |
0.972 BTU-in/hr-ft²-°F @Temperature 900 °F |
|
3M Interam™ E-5A-4 Endothermic Mat When properly installed, 3M Interam Endothermic Mat E-5A-4 provides a uniform covering that, when exposed to high temperatures, releases chemically-bound water to cool the outer surfaces of the wrap.. |
|||
Thermal Conductivity | 0.140 W/m-K @Temperature 1100 °C |
0.972 BTU-in/hr-ft²-°F @Temperature 2010 °F |
|
Zircar Zirconia ZYC Zirconia Cylinders Insulation Zircar Zirconia Cylinders Type ZYC are rigid, free standing refractory structures composed of yttria stabilized zirconia fibers that are bonded with silica. The material is evenly bonded, allowing .. |
|||
Thermal Conductivity | 0.140 W/m-K @Temperature 800 °C |
0.972 BTU-in/hr-ft²-°F @Temperature 1470 °F |
ASTM C177-76 |
Zircar Ceramics ASH Alumina-Silica Insulation ZIRCAR Ceramics Alumina-Silica Insulation Type ASH is one of the first alumina-silica products produced by ZIRCAR. Made of bulk fiber and inorganic alumina binders Type ASH is uniform throughout its.. |
|||
Thermal Conductivity | 0.140 W/m-K @Temperature 871 °C |
0.972 BTU-in/hr-ft²-°F @Temperature 1600 °F |
|
Zircar Refractory Composites ASPA-1 Alumina-Silica Fiber Paper ASPA-1 is a premium grade, lightweight refractory material made from high purity alumina-silica fibers formed into highly flexible sheets. This alumina-silica fiber paper exhibits very low thermal c.. |