Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Duratherm 600 Paraffinic Heat Transfer Fluid

Category Fluid
Manufacturer Duratherm
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Duratherm 600 Paraffinic Heat Transfer Fluid.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Duratherm 600 - thermal fluid rated to 600°F it contains the industries most aggressive blend of additives for long, trouble free operation in a variety of applications. Specifically engineered to withstand the extreme oxidation environment in open systems such as extrusion, blow molding and electrically heated portable systems as well as many others. A proprietary dual stage anti-oxidant system, seal and gasket extender as well as numerous other additives ensures a cleaner, longer running fluid.Information provided by Duratherm.
Physical Properties Metric English Comments
Specific Gravity 0.868 g/cc
0.868 g/cc
at 60°F
Density 0.662 g/cc

@Temperature 316 °C
0.0239 lb/in³

@Temperature 600 °F
0.676 g/cc

@Temperature 288 °C
0.0244 lb/in³

@Temperature 550 °F
0.702 g/cc

@Temperature 260 °C
0.0253 lb/in³

@Temperature 500 °F
0.731 g/cc

@Temperature 204 °C
0.0264 lb/in³

@Temperature 400 °F
0.851 g/cc

@Temperature 37.8 °C
0.0307 lb/in³

@Temperature 100 °F
Kinematic Viscosity 0.75 cSt

@Temperature 260 °C
0.75 cSt

@Temperature 500 °F
0.83 cSt

@Temperature 260 °C
0.83 cSt

@Temperature 500 °F
0.95 cSt

@Temperature 260 °C
0.95 cSt

@Temperature 500 °F
Kinematic Viscosity at 40°C (104°F) 32.1 cSt
32.1 cSt
Kinematic Viscosity at 100°C (212°F) 5.2 cSt
5.2 cSt
Molecular Weight 372 g/mol
372 g/mol
Average
Vapor Pressure 0.0269 bar

@Temperature 204 °C
20.1 torr

@Temperature 400 °F
0.0379 bar

@Temperature 260 °C
28.4 torr

@Temperature 500 °F
0.07860 bar

@Temperature 288 °C
58.95 torr

@Temperature 550 °F
0.1531 bar

@Temperature 316 °C
114.8 torr

@Temperature 600 °F
Thermal Properties Metric English Comments
Specific Heat Capacity 1.97 J/g-°C

@Temperature 37.8 °C
0.470 BTU/lb-°F

@Temperature 100 °F
2.51 J/g-°C

@Temperature 204 °C
0.600 BTU/lb-°F

@Temperature 400 °F
2.68 J/g-°C

@Temperature 260 °C
0.640 BTU/lb-°F

@Temperature 500 °F
2.76 J/g-°C

@Temperature 288 °C
0.660 BTU/lb-°F

@Temperature 550 °F
2.89 J/g-°C

@Temperature 316 °C
0.690 BTU/lb-°F

@Temperature 600 °F
Thermal Conductivity 0.126 W/m-K

@Temperature 316 °C
0.876 BTU-in/hr-ft²-°F

@Temperature 600 °F
0.128 W/m-K

@Temperature 288 °C
0.888 BTU-in/hr-ft²-°F

@Temperature 550 °F
0.130 W/m-K

@Temperature 260 °C
0.900 BTU-in/hr-ft²-°F

@Temperature 500 °F
0.133 W/m-K

@Temperature 204 °C
0.924 BTU-in/hr-ft²-°F

@Temperature 400 °F
0.140 W/m-K

@Temperature 37.8 °C
0.972 BTU-in/hr-ft²-°F

@Temperature 100 °F
Pour Point -10.0 °C
14.0 °F
Flammability Test 464
464
Fire Point, °F
680
680
Autoignition Temp, °F
Flash Point 224 °C
435 °F
Descriptive Properties Value Comments
Distillation range at 10% 715
Distillation Range at 90% 886
Max Bulk Temp (°F) 600
Max Film Temp (°F) 650
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved