Material Notes:
ASPA-880 is a high temperature, lightweight refractory material made from alumina-silica fibers formed into highly flexible sheets. It is made from shorter and smaller diameter fibers with a higher alumina content and are laid up at significantly higher density. These factors lead to high temperature, slow shrinkage, higher strength, and better chemical resistivity. This alumina-silica fiber paper exhibit very low thermal conductivity and is designed for use in applications where flexibility, high strength and resistance to heat are paramount. Type ASPA-880 exhibits low thermal conductivity and is ideal for applications up to 1450°C (2642°F). It is used in environments where standard ceramic fiber papers will not survive.Information provided by ZIRCAR Refractory Composites, Inc. (ZRCI)
Physical Properties Metric English Comments
Density 0.280 g/cc
0.0101 lb/in³
Loss On Ignition 8.0 %
8.0 %
Thermal Properties Metric English Comments
Thermal Conductivity 0.0800 W/m-K

@Temperature 500 °C
0.555 BTU-in/hr-ft²-°F

@Temperature 932 °F
0.120 W/m-K

@Temperature 800 °C
0.833 BTU-in/hr-ft²-°F

@Temperature 1470 °F
0.140 W/m-K

@Temperature 871 °C
0.972 BTU-in/hr-ft²-°F

@Temperature 1600 °F
0.160 W/m-K

@Temperature 1100 °C
1.11 BTU-in/hr-ft²-°F

@Temperature 2010 °F
Melting Point 1930 °C
3510 °F
Maximum Service Temperature, Air 1450 °C
2640 °F
Component Elements Properties Metric English Comments
Al2O3 55 %
55 %
Other 1.0 %
1.0 %
SiO2 44 %
44 %
Descriptive Properties Value Comments
Color White
Fiber Index, % 45
Mullen Burst, psi 37
Tensile Strength, g/in 6500
Type of Binder Organic