Description: Golite 95 is widely applied as an insulating backlining behind a dense castable, especially in the petrochemical industry.Remarks: These values apply to cast products. Also available in gunning variety, marked "GM".Information provided by Gouda Vuurvast.
Physical Properties Metric English Comments
Bulk Density 0.700 - 0.760 g/cc
0.0253 - 0.0275 lb/in³
After drying at 110°C
Particle Size <= 4000 µm
<= 4000 µm
Grain Size
Mechanical Properties Metric English Comments
Compressive Strength 1.50 - 2.50 MPa

@Temperature 950 °C
218 - 363 psi

@Temperature 1740 °F
Cold Crushing Strength
2.50 - 3.50 MPa

@Temperature 100 °C
363 - 508 psi

@Temperature 212 °F
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 0.140 - 0.220 W/m-K

@Temperature 100 °C
0.972 - 1.53 BTU-in/hr-ft²-°F

@Temperature 212 °F
0.180 - 0.260 W/m-K

@Temperature 600 °C
1.25 - 1.80 BTU-in/hr-ft²-°F

@Temperature 1110 °F
0.220 - 0.300 W/m-K

@Temperature 950 °C
1.53 - 2.08 BTU-in/hr-ft²-°F

@Temperature 1740 °F
Maximum Service Temperature, Air 950 °C
1740 °F
Shrinkage -4.00 - 1.00 %

@Temperature 950 °C
-4.00 - 1.00 %

@Temperature 1740 °F
Permanent Linear Change
Component Elements Properties Metric English Comments
Al2O3 12 %
12 %
SiO2 34 %
34 %
Descriptive Properties Value Comments
ASTM Classification N
Material Consumption per 1 m3 625 kg
Mixing Water 70-80 liters
per 100 kgs dry material